Ceramic Industry
  Home
  Subscribe
  Digital Edition Subscribe
  CyberNews Subscribe
  Editor's Blog
  PPP HotSpot
  Subscription Customer Service
  Online
  Classified Ads
  Services Marketplace
  Buyers' Connections
  Ad Index
  Calendar
  Today's Headlines
  Cover Story
  Features
  Columns
  Products
  Online Extras
  Resources
  Archives
  Digital Edition Archives
  Career Center
  CyberNews Archives
  Advanced Ceramics & Glasses Digest eNews Archives
  Directories
  Videos
  Podcasts
  Reference
  Market Research
  Web Seminars
  CI Info
  About CI
  Contact Us
  Media Kit
  Reprints
Search in: EditorialProductsCompanies
Investing In Ceramics: JM Plans for Bright Future


September 28, 2000

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare





In 1998, Johnson Matthey (JM) acquired the Cookson Matthey joint venture and introduced plans to build a new opacifier manufacturing facility in Jacksonville, Fla. The company chose Jacksonville for several reasons, including its proximity to raw material sources, excellent transportation and closeness to a deep-water port.

The new JM plant is located within 40 miles of both the Iluka and DuPont heavy mineral mines, and it provides trucks easy highway access. Jacksonville's port at Blount Island handles significant container cargo, and the Port of Jacksonville is developing bulk handling. The location allows JM to minimize its transportation both into the factory and ultimately to the customer.

Johnson Matthey broke ground on this greenfield site in May 1999. Site work, underground utilities and development of foundations began immediately. Ball mills, classification equipment, dust collectors, silos and packing equipment began arriving in early September, and equipment installation and building construction proceeded at an accelerated pace through October and November. On December 17, the first milled zircon produced in the Jacksonville facility exited the mill.

From early January until February 14, 2000, plant personnel worked to debug the new process. Particle size testing was done both in the U.S. and in the company's New Castle, U.K., facility. Other tests, including chemistry and firing glaze samples, were performed in the U.K.

By February 15, JM was ready to show off the plant, and the company held an open house for several key ceramic industry decision-makers, as well as City of Jacksonville officials.

A key part of the new facility is its processing technology. This is the first JM site dedicated to manufacturing opacifiers through lower-cost, proprietary, dry processing technologies rather than the wet process, which is largely used in the other eight JM zircon processing sites. The manufacturing process was internally designed by JM personnel, who collectively have a long history of manufacturing and innovation in the production of opacifiers.

The goal during start up was to produce opacifiers using the new technology with performance equal to the company's Zircopax Plus and Superpax Plus products. The start up went very smoothly, and by mid-February the plant was producing-via the wet process-opacifiers almost identical in performance to Zircopax Plus.

Samples have been sent to many customers and the feedback has been positive. In April, the new facility began shipping Zircopax Plus, and most of the company's customers are now buying U.S. produced Superpax Plus and Zircopax Plus products. Future expansions are likely as U.S. demand increases for JM's opacifier products.

In addition to housing the opacifier business, JM supports accounting, administration and customer service for its Structural Ceramics Division at the Jacksonville facility. The Structural Ceramics business supplies glazes, grits, stains, etc. to tile and sanitaryware manufacturers in North America.



For More Information

For additional information about Johnson Matthey or its products, contact Dan Rooney, 11400 New Berlin Rd., Jacksonville, FL 32226, (904) 751-2828, fax (904) 751-6828.