Ceramic Industry
  Home
  Subscribe
  Digital Edition Subscribe
  CyberNews Subscribe
  Editor's Blog
  PPP HotSpot
  Subscription Customer Service
  Online
  Classified Ads
  Services Marketplace
  Buyers' Connections
  Ad Index
  Calendar
  Today's Headlines
  Cover Story
  Features
  Columns
  Products
  Online Extras
  Resources
  Archives
  Digital Edition Archives
  Career Center
  CyberNews Archives
  Advanced Ceramics & Glasses Digest eNews Archives
  Directories
  Videos
  Podcasts
  Reference
  Market Research
  Web Seminars
  CI Info
  About CI
  Contact Us
  Media Kit
  Reprints
Search in: EditorialProductsCompanies
Lux Research Report Finds Nanotechnology on the Rise (posted 7/24/08)

July 24, 2008

ARTICLE TOOLS
EmailEmailPrintPrintReprintsReprintsshareShare



Much like the Internet, nanotechnology was over-hyped earlier this decade, and some high-profile failures left manufacturers and investors skeptical. However, a new report from Lux Research finds that, in reality, nanotechnology has become pervasive in a wide range of industries. In 2007, $147 billion worth of nano-enabled products were produced, a figure set to grow to $3.1 trillion in 2015.

“Nanotech isn’t a new market or industry—it’s an enabling technology that improves many types of products,” said Jurron Bradley, Ph.D., senior analyst at Lux Research. “For example, you find it in coatings boosting the efficiency of automobile engines, in nano-enabled finishes protecting electronic devices, and in nanoparticulate reformulations that make cholesterol-reducing drugs more effective. These innovations aren’t always visible to consumers, but they improve products and boost margins. That’s why nanomaterials’ use is only going to keep growing.”

To gauge nanotech’s commercial impact, Lux Research used its value chain framework to measure and forecast adoption across three major industry sectors (manufacturing and materials, electronics and IT, and healthcare and life sciences) in the U.S., Europe, Asia/Pacific and the rest of the world from 2004 to 2015. The nanotechnology value chain begins with nanomaterials, which are nano-scale bits of matter with unique size-dependent properties. These nanomaterials are then incorporated into nanointermediates, such as coatings or memory chips, which are in turn used to make nano-enabled final products ranging from airplanes to cell phones to medical diagnostics. This forecast draws on data from over 1000 primary interviews that Lux Research analysts conduct with technology developers annually, as well as a new survey of 31 leading corporations active in nanotechnology.

The materials and manufacturing sector saw the greatest impact in 2007, incorporating nanotechnology in $97 billion in products across the value chain as nanotech made its way into intermediates like coatings and composites for products like automobiles and buildings. Electronics followed at $35 billion from emerging nanotech applications in fields like displays and batteries, while healthcare trailed with $15 billion in revenue, driven by pharmaceutical applications.

Electronics applications of emerging nanotechnology will gain ground through 2015, growing at a 51% compound annual growth rate (CAGR) to reach $940 billion, while healthcare and life sciences will grow at 46% annually to reach $31 billion. However, the materials and manufacturing sector will remain predominant, growing at 45% to reach $1.8 trillion worth of product revenue incorporating emerging nanotech.

Nanotech’s greatest economic impact is currently in the U.S., where companies incorporated nanotech into $59 billion in products in 2007. Europe followed at $47 billion, Asia/Pacific accounts for $31 billion and the rest of the world for $9.4 billion. However, Europe’s steeper CAGR of 48% will bring it to $1.09 trillion by 2015, meeting the U.S.’s $1.08 trillion, and Asia will remain in third place at $717 billion.

Nanotechnology R&D hit $13.5 billion in 2007, up 14% from 2006. Global corporate R&D spending grew 23% to reach $6.6 billion, passing government spending for the first time and dwarfing VC investments. “Nanotech’s broadening impact will touch more final product categories over the next four years,” said Michael Holman, research director at Lux Research. “Past 2012, however, nanotech’s impact will primarily deepen as new nanotech innovations get incorporated into product categories that already make use of existing nanotech enhancements. It’s during this later time frame that more disruptive innovations like new types of nano-enabled memory chips will begin to make their presence felt.”

The 135-page report includes projections on the value of products incorporating nanotechnology across the value chain from 2004 to 2015, broken down by value chain stage, industry sector and region. It offers a concise introduction to nanotechnology, as well as profiles of 10 major nanomaterials like carbon nanotubes and quantum dots, and 10 major nanointermediates like nano-enabled coatings and drug delivery systems. The report also includes a detailed analysis of nanotechnology funding from corporations, governments and venture capitalists; discussions of key issues for environmental, health and safety (EHS); information regarding how large corporations are approaching nanotechnology; and the prospects for nanomaterials start-ups and other specialists.

“Nanomaterials State of the Market Q3 2008: Stealth Success, Broad Impact” is part of the Lux Research Nanomaterials Intelligence service. For information on how to become a client, call (646) 649-9582 or e-mail john.schwartz@luxresearchinc.com. The company’s website is located at www.luxresearchinc.com.