BLASCH ACHIEVEMENT AWARD GIVEN TO BRIAN MACINTOSH The Precision Ceramics Achievement Award is given to the employee who best shows achievement of personal and company-wide goals.
FULL STORY
BORAL BRICKS PLANT RECEIVES LEED GOLD RATING Boral Bricks Inc.'s Terre Haute, Ind., manufacturing facility has received Leadership in Energy and Environmental Design Gold certification from the USGBC.
FULL STORY
CAROMA USES SACMI E-LEARNING PROJECT Sacmi announced that its e-learning project is being used by Caroma. The project began in 2003 for the training and maintenance of the company's machines.
FULL STORY
|
|
|

CI LinkedIn Group Continues to Grow
The Ceramic Industry magazine group on LinkedIn offers a forum for anyone involved in the ceramic, glass and related industries. The group provides opportunities for discussion, news and information sharing, and networking with other industry professionals. We'd love for you to join us!
|
|
|
FERRO EXPANDS PV TECHNOLOGY CENTER CAPABILITY IN ASIA Ferro Corp. announced plans to expand capability in two of its Asian PV technology centers as part of an effort to support growth in that market.
FULL STORY
NYCO ANNOUNCES PRICE ADJUSTMENT
NYCO Minerals and its affiliate divisions will increase prices
for all wollastonite products produced from the New York and Mexican
Operations by 6-8%.
FULL
STORY
OWENS CORNING NAMES DIRECTOR OF BUILDING SCIENCE Owens Corning has appointed Achilles Karagiozis director of Building Science. He is based in the company's Granville, Ohio, Science and Technology Center.
FULL STORY PANALYTICAL INTRODUCES DIFFRACTOMETER PANalytical has launched an Empyrean high-performance diffractometer, which offers a 3-D detection system that enables it to measure all sample types.
FULL STORY
RIO TINTO TO INVEST $469 MILLION IN MICH. MINE Rio Tinto has announced plans to invest $469 million in constructing the Kennecott Eagle nickel and copper mine in Michigan's Upper Peninsula.
FULL STORY
SAINT-GOBAIN SUBSIDIARY TO BUILD SECOND PV PLANT Saint-Gobain subsidiary Avancis will build a new plant to make PV modules to cover the roofs of buildings, as well as solar plants.
FULL STORY
|
|
|
 |
|  |
| | | |
| |
|
Career Center
Are you in the job market? CI can help! Our online classified ads showcase the latest job openings and opportunities.
Online Calendar CI's full Calendar of Events is available online to help you keep track of all the latest trade shows and seminars. |
|
|
CyberTip Looking for more? CI's website features dozens of additional stories that we don't have room for in CI CyberNews or in print issues. Whether you're looking for additional industry news, personnel announcements or new product technologies, we've got it all online at
www.ceramicindustry.com! |
|
| |
Survey Says!
Last week's CI CyberNews CyberPoll asked if the Gulf Coast oil spill had impacted our readers' businesses. All of the respondents (100%) answered no. One reader commented, "However, it is just a matter of time before the government will impact our business [by] saying the oil spill is everyone's responsibility."
Follow this link to share your thoughts on this topic.
|
|
| | |
|
CHARTER SPONSOR
Mohr Corp. provides ceramic and machinery services to both buyer and seller, from the sale of one machine to entire factories, with its professionally established brokering, liquidation and appraisal organization. For more information, visit www.mohrcorp.com. |
|
ABOUT OUR SPONSOR
Insaco is a precision machining company that provides finished pieces to customers' specifications from ultra hard materials, including oxide ceramics, nitrides, carbides and quartz, and especially industrial sapphire. NEW capability allows the company to machine within a 102" x 31" x 70" envelope and still hold tight tolerances. Visit www.insaco.com. |
| All statements about the companies/products included in this newsletter are manufacturers' claims, and neither CI CyberNews nor Ceramic Industry endorses any of the products mentioned. |
|
Copyright © 2010 by BNP Media. All Rights Reserved. |
|
| | | | |
| BNP Media 2401 W. Big Beaver Road, Ste. 700 Troy, Michigan 48084-3333 U.S.A. | |
|
| |
|
| |
| |
|