Ceramic Industry News

HED Calcining Furnace Upgrade Doubles Production

HED International recently commissioned an upgrade of a calcining furnace in Charleston, S.C., with the addition of a new combustion system, a ceramic muffle, PLC and touchscreen HMI control panel. "The result is a furnace that is performing great; firing uniformity is excellent," said John Steele, HED project manager. "We're pleased that production has doubled without much more fuel consumption, and everyone is breathing a lot easier now that the air is cleaner because dusting is no longer a problem from this furnace."

For more information, call (609) 466-1900, fax (609) 466-3608, e-mail info@hed.com or visit http://www.hed.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!