BCR: MACT Solutions

Although the final MACT rule has yet to be published, companies should start preparing now to meet the new regulations.

A DIFF scrubbing system at Boral Bricks’ Plant 4 in Augusta, Ga. Photo courtesy of Procedair Industries, Englewood, Colo.
On July 22, 2002, the U.S. Environmental Protection Agency (EPA) published the proposed National Emission Standards for Hazardous Air Pollutants (NESHAP) for Brick and Structural Clay Products Manufacturing and Clay Ceramics Manufacturing, commonly known as the “MACT rule.” The rule will require major sources of hydrogen fluoride (HF), hydrogen chloride (HCl) and metals (controlled as particulate matter [PM]) to meet emission standards using a Maximum Achievable Control Technology (MACT). According to the proposed rule, plants that own or operate an existing tunnel kiln with a design capacity equal to or greater than 9.07 megagrams per hour (Mg/hr) (10 tons per hour [tph]) or a new or reconstructed tunnel kiln, regardless of capacity, will be required to meet an HF emission limit of 0.027 pound per ton (lb/ton) of product or reduce uncontrolled HF emissions by at least 95% for affected process streams. They would be required to meet an HCl emission limit of 0.037 lb/ton of product or reduce uncontrolled HCl emissions by at least 90%. And they would be required to meet a PM emission limit of 0.12 lb/ton of product.

The final rule is expected to be published in the Federal Register in early to mid-2003. Companies with existing tunnel kilns that are subject to the rule will have three years from the time the final rule is published in the Federal Register to comply, so it’s possible that compliance might not be required until 2006. However, any company that constructed a new tunnel kiln or revamped its existing kilns after July 22, 2002, will need to comply with the final rule as soon as it is published. Additionally, any company that is planning a plant expansion or a kiln revamp in 2003 will need to be in compliance upon initial startup of their kiln(s).

The “MACT hammer” might further complicate the situation. This issue arose when the EPA missed the November 18, 2000, deadline mandated by the Clean Air Act to issue nationwide MACT standards for hazardous air pollutants (HAPs). Without the new provisions of the MACT final rule, state and local governments were to begin setting their own emissions standards on a case-by-case basis 18 months after the deadline (May 15, 2002). Under the MACT hammer provision, facilities would also be required to submit detailed permit applications to states so that state-permitting agencies could determine MACT standards for each individual facility. Although this requirement has not yet been triggered on a national level, some states have already begun the permit application process, and companies in these states could be forced to comply with strict emission standards as early as 2004.

The Brick Industry Association (BIA) Task Force and other industry groups are continuing to lobby for changes to the final rule, and many brick manufacturers have decided to take a “wait and see” approach. However, while it may be wise to hold off on purchasing the actual control technology, companies can begin taking a number of steps now to ensure that they will be prepared to meet the new regulations.

Educate Yourself

The proposed MACT rule lists several types of air pollution control devices (APCDs) that are currently used to control emissions, including dry lime injection fabric filters (DIFF), dry lime scrubber/fabric filters (DLS/FF), dry limestone adsorbers (DLA), wet scrubbers (WS) and fabric filters.

Despite the EPA’s apparent endorsement of some of these systems in the proposed rule, not all APCDs have been proven to remove the required level of pollutants. Additionally, what works for one plant might not be the right solution for another facility. According to Lars Hansen, sales manager for Procedair Industries, Englewood, Colo., one of the most important things companies can begin doing right now is educating themselves about the MACT rule and the various options for compliance.

“Companies should contact different scrubber vendors and have them visit their plants and give presentations so they can educate themselves. Most suppliers will be happy to come and help them in that process,” Hansen said.

Independent consultants can also help companies ensure that they select the right type of control device. “When companies are evaluating different technologies, it can be difficult to maintain an objective viewpoint. An independent reviewer can help guide the equipment selection process and ensure that the proper level of control is selected,” said Andy Turnbull, president of Lucas Process Systems in Charlotte, N.C.

Prototypes of this wet scrubber system have been successfully tested in the brick industry. Photo courtesy of CECO Filters, Conshohocken, Pa.

Evaluate Your Plant’s Needs

Of course, the most important criterion for any APCD is whether it meets the final MACT standards. Beyond that, however, the type of APCD selected will most likely depend on a given plant’s operating parameters and waste disposal options. For example, some wet scrubbers might require up to 20 gallons of water per minute to operate, with a discharge rate of up to 1 gallon per minute. Companies with access to ample water supplies and the ability to use a local sewer for wastewater might find a wet scrubber to be the ideal solution, while companies that cannot discharge liquid waste or do not have access to a significant amount of water at the plant might decide to go with a dry scrubber. However, according to Fred Mueller, industry business manager with CECO Filters, Conshohocken, Pa., the situation might not be quite that easily defined.

“Companies that can’t tolerate a liquid discharge but still want to use a wet scrubber have some options,” Mueller said. “For example, in one CECO system that is being installed right now, a specialty filter dewaters scrubber sludge so that the liquid waste is cleaned of practically all solids. The remainder is a dry waste, which can go to a landfill. For companies that can’t tolerate any liquid waste, a spray dryer can also be used.”

Operating flexibility is another issue to consider. “Companies need to look at the operating range of any scrubber they’re considering, and also look at the operating range at which they run their tunnel kiln,” recommends Don Denison, president of Denison Engineering and a representative for ENCERTEC, Inc. “When times are hard, it’s common for tunnel kilns to run at half, or even a third of their speed, so companies need to have a scrubber that can handle the slower speeds, as well as high speeds for times when plants are running at full capacity. Not all scrubbers can meet that level of flexibility.”

The amount of support a company needs from its vendor might also be a factor in the decision-making process. Some suppliers offer complete turnkey installations, including everything from the initial system design, to handling all of the necessary components and access platforms, to employee training and startup of the final system. While this option can be more expensive, it provides a “one-stop solution” for companies with few in-house resources. Companies that have their own environmental and engineering teams on staff or that want to become more involved in the process might prefer to purchase a simpler system and handle some of the work themselves.

Begin Budgeting for Compliance

No one wants to think about the impact the new rule will have on the bottom line. Unlike other capital investments, a new APCD has no “payback,” unless you consider the potential cost of penalties for noncompliance. Still, with typical systems running anywhere from $500,000 to $1 million, companies would do well to begin budgeting now, even before the final rule goes into effect.

According to Fred Mueller from CECO Filters, the initial cost of an APCD is going to be governed by 1) the amount of HAPs in the stack emissions; 2) whether any discharge treatment from the scrubber system is required (e.g., filters and spray dryers for wet systems); and 3) the kiln capacity. “In general, the higher the emissions and the larger the kiln, the higher the cost of the scrubber system,” Mueller said.

However, cost isn’t always proportional to capacity. With many scrubbers, there are some economies of scale. “The cost starts slowing down with the larger kiln sizes (above 50 to 70 million standard brick equivalent [SBE] per year) because there are a lot of components—instrumentation, piping, auxiliary, controls, etc.—that are pretty much fixed, regardless of size. The building that houses the scrubber is also generally fixed, and as the size of the scrubber goes up, that structure wouldn’t change too much. So the cost increase [for companies operating at capacities above 70 million SBE] would be insignificant,” Mueller said.

Look Beyond First Cost

While the initial cost of an APCD is an important factor, it isn’t the only cost to consider when evaluating the different systems. According to Lars Hansen of Procedair, the operating cost of a scrubber is just as important as the first cost—if not more so.

“Companies don’t want to spend a lot of money for something that doesn’t improve production or help their bottom line, so it can be appealing to buy the lowest-cost technology they can find. But in many cases, they will end up spending more money in the long run by buying something cheaper, either because they’ll have to do it over or they’ll have to constantly deal with problems,” Hansen said.

Plants should consider factors such as power consumption, the cost of fresh reagent (or water) and the cost to dispose of the waste reagent (or wastewater). Many suppliers will compile detailed operating cost data upon request. There can also be a number of “hidden costs” that should be taken into account. For example, the types of controls will vary from system to system, with the more sophisticated controls likely carrying a higher price tag. With higher-priced turnkey installations, employee training, initial startup and troubleshooting are generally part of the package.

“When plants compare proposals, it is important that they look at all of these details to find out where the differences really are,” Hansen said.

Simplify, Simplify, Simplify

Although it can be tempting to assemble an APCD “piecemeal” from various suppliers and in-house components to try to save on the initial cost, buying a system as a total package can greatly simplify the process, saving time and money in the long run.

“I don’t want to simply provide someone with an erector set because if something goes wrong, it can be difficult to pinpoint and resolve the problem. If the system is provided as an entire package, only one supplier is responsible for solving the problem,” said Fred Mueller from CECO Filters.

However, Andy Turnbull from Lucas Process Systems cautioned that companies should be sure to select services that are suited to the vendor rather than trying to force a business relationship that is not well suited to either party. “Brick manufacturers often assume that all vendors provide a turnkey approach, when in fact many are smaller, device-oriented specialists. Companies need to keep in mind that additional items such as installing the foundation or supplying a stack, for example, are not always a part of the air pollution vendor’s scope, and they can often save a significant amount of money if a team approach is used.”

Develop a Partnership with Suppliers

For many plants, the cost of compliance to the new rule—especially when factoring in overall operating costs—will seem quite staggering. Preventing these costs from adversely affecting the long-term competitiveness of brick in the paver and construction markets will require a concerted effort among manufacturers and scrubber suppliers.

“Many companies are just looking for vendors to give them a price—they don’t want to take any ownership of the situation. Instead, the industry as a whole needs to be collectively looking at and working with vendors to refine options and find ways to save money,” said Turnbull.

Work Closely with State Regulatory Agencies

State regulatory agencies will ultimately be responsible for setting and enforcing the final MACT rule. While few people enjoy working closely with government officials, it is far better to be proactive than reactive when it comes to environmental issues. According to Lars Hansen from Procedair, companies can often get themselves in trouble simply by not following deadlines.

“It is important to follow the rules that the local agencies have set up and to send in any required reports on time. Not doing so can create a number of problems, including potential fines,” Hansen said.

Additionally, since states will have the flexibility to mandate stricter standards than those published in the final MACT rule, companies should try to go beyond minimum compliance efforts. “Some states—Texas, for example—have taken the attitude that sulfur needs to be controlled as well, even though that isn’t part of the federal standard. Companies should be prepared to be held to stricter controls than what the federal MACT is mandating,” Hansen said.

Keep an Open Mind

As the new MACT rule becomes a reality, plants will begin hearing more and more advice on how they can comply, as well as testimonials from companies who have already gone through the compliance process. But don’t take anyone’s word for it. Educate yourself, evaluate your plant’s needs, begin budgeting early for compliance, look beyond the first cost of the different control options, choose the simplest practical solution, develop a partnership with APCD suppliers and work closely with state regulatory agencies. Above all, keep an open mind about the different options for compliance, and make sure the system you choose meets the anticipated emission standards. When it comes to MACT, there is no one-size-fits-all answer. The best solution is simply the one that is right for your plant.

For More Information

For more information about APCDs, contact:
  • Bionomic Industries, 777 Corporate Dr., Mahwah, NJ 07430; (201) 529-1094; fax (201) 529-0252; www.bionomicind.com.
  • CECO Filters, 1029 Conshohocken Rd., Conshohocken, PA 19428; (800) 220-8021 or (610) 825-8585; fax (610) 825-3108; e-mail fmueller@cecofilters.com or sales@cecofilters.com; www.cecofilters.com
  • Danser, Inc., Vacuduct Div., Rt. 50, Murphytown Rd., P.O. Box 4098, Parkersburg, WV 26104; (304) 679-3666; fax (304) 679-3354; e-mail sales@danserinc.com; www.danserinc.com
  • ENCERTEC, Inc., 3859 Battleground Ave, Suite 205, Greensboro, NC 27410; (336) 288-7226; fax (336) 288-5994; e-mail encertec@aol.com
  • Hellmich GmbH & Co. KG, Holt Kamp Weg 13, 32278 Kirchlengern, Germany; (49) 5223-75770; fax (49) 5223-757730; e-mail info@hellmich.com; www.hellmich.com
  • Kirk & Blum, P.O. Box 35423, Greensboro, NC 27425; (336) 668-3773; fax (336) 668-9779; e-mail jfinn@kirkblum.com; www.kirkblum.com
  • Lucas Process Systems, 10800 Sikes Place, Suite 160, Charlotte, NC 28277; (704) 321-2552; fax (704) 321-2554; e-mail lucas@lucasprocess.com; www.lucasprocess.com
  • Solios Environment (prev. Procedair Industries), 6860 S. Yosemite Ct., Suite 2204, Englewood, CO 80112; (303) 713-022; fax (303) 713-9131; e-mail l.Hansen@solios.com; www.solios.com
  • Tri-Mer Corp., P.O. Box 730, Owosso, MI 48867-0730; (989) 723-7838; fax (989) 723-7844; e-mail salesdpt@tri-mer.com; www.tri-mer.com
Editor’s note: This is not a complete list. If your company supplies scrubbers to the brick industry and would like to be added to this list, please contact the Editor at grahlk@bnp.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Recent Articles by Christine Grahl

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!