New Products / Product Highlights

Aremco Products, Inc.: Black Ceramic Coating

HiE-Coat(TM) 840-C, a black, water-based ceramic coating, is now available from Aremco Products, Inc.

HiE-Coat(TM) 840-C, a black, water-based ceramic coating now available from Aremco Products, Inc., demonstrates an emissivity greater than 0.90 at temperatures to 2500F. The emissivity of a material can range from 0.00 to 1.00; a high emissivity material will absorb and effectively re-radiate infrared energy. High-temperature combustion chambers, ovens and furnaces constructed using high-emissivity coatings are more energy efficient and can distribute heat more uniformly. HiE-Coat 840-C is applied to ceramic and refractory surfaces using a sponge brush, roller or conventional spray equipment. The coverage rate is approximately 500 ft(2)/gallon, based on 2 mil dry film thickness. Curing is accomplished in operation or by heating for 1-2 hours at 200F.

For more information, call (845) 268-0039, fax (845) 268-0041, e-mail aremco@aremco.com or visit http://www.aremco.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!