PRODUCT PROFILE: High Throughput with a Fine Grind

April 1, 2005
/ Print / Reprints /
ShareMore
/ Text Size+
A new jet mill combines a spiral design with a patented dynamic air classifier wheel to achieve optimum levels of fineness and throughput.

The high-density bed jet mill.
Jet mills-including designs such as spiral, loop, opposed and fluidized bed-are commonly used in the ceramic industry to produce the superfine powders required for many high-tech applications. The mills pulverize materials in a chamber by propelling particles into each other and into the chamber wall or an impact plate at high velocities using multiple jets of air or steam. Because size reduction is the result of high-velocity collisions between particles of the process material rather than collisions with grinding media, jet mills virtually eliminate the risk of contamination or attritional heat, making them ideal for high-purity and/or heat-sensitive materials.

However, conventional jet mills have had some drawbacks. For example, in spiral and loop jet mills, the level of fineness that can be achieved depends on the feed rate; higher feed rates produce coarser powders. This forces manufacturers to choose between a high level of throughput or the fineness of grind. In opposed and fluidized bed jet mills, the level of fineness that can be achieved is a function of the classifier tip speed and airflow. However, most classifiers are also limited in their ability to handle high throughput levels at a fine particle size distribution.

Recently, a new high-density bed jet mill* has been introduced that combines the best aspects of spiral jet milling with an advanced air classifier to offer precise particle size control at high throughput levels.

*The NETZSCH-CONDUX(r) Conjet high density bed jet mill, supplied by NETZSCH-CONDUX Maltechnik GmbH, Hanau, Germany, and Netzsch Fine Particle Technology, LLC, Exton, Pa.

Spiral Jet Limitations

To understand how the new jet mill works, it is first helpful to understand the limitations of a conventional spiral jet mill related to classification. In powder processing, classification is generally defined as the separation of bulk materials according to their settling velocity in a fluid (usually a gas, but sometimes a liquid). It is used to separate heavy particles from lighter particles, high aspect ratio particles from round particles, and/or fine particles from coarse particles. The settling velocity depends on the particle shape, density and size, as well as the fluid viscosity and density. External classification is used in many grinding operations (e.g., ball mill systems often use external classifiers in mineral processes), while internal classification is used in mechanical air classifier mills or fluidized bed jet mills to control the maximum particle size.

Conventional spiral jet mills feature an internal static air classifier that operates on a free vortex principle-i.e., both the feed material and air jets enter the classifier tangentially and are drawn into the classifier by a downstream exhaust fan. Coarse particles, influenced by the mass force (a function of their velocity as they enter the classifier), migrate to the periphery of the spiral jet mill, where they undergo collisions to be reduced in size. Fine particles, which are influenced by the drag force imparted by the fluid, are carried out with the fluid to be conveyed tto a downstream collector.

The only way to decrease the particle size exiting the mill is to increase the force of the air jets, thereby increasing energy consumption, or to decrease the amount of feed material entering the mill, thereby reducing throughput. However, even at lower throughput levels, the resulting particle size distribution is not exact. The higher airflow needed to achieve a smaller particle size often creates additional fines, and some coarse particles are allowed to exit the mill into the product stream.

Figure 1. Operation of a fluidized bed jet mill.

Fluidized Bed Improvements

To avoid the classification problems found with a spiral jet mill, some companies use fluidized bed jet mills (see Figure 1). A fluidized bed jet mill has high-pressure gas nozzles positioned around the mill housing. The high-velocity gas jets from the nozzles accelerate particles up to 540 meters per second (depending on pressure and temperature), and size reduction is a result of inter-particle collision. Unlike the free vortex classification of a conventional spiral jet mill, classification in a fluidized bed jet mill operates on a forced vortex principle, in which mass force is exerted by the peripheral velocity of a mechanical classifier wheel. Coarse particles, influenced by the mass force, are rejected back to the milling chamber, while fine particles, influenced by the drag force imparted by the fluid, are carried with the fluid through the classifier wheel.

Increasing the peripheral velocity of the classifier wheel increases the mass force on the particles, rejecting more particles and resulting in a finer fines fraction. Conversely, increasing the airflow through the classifier wheel increases the drag force in the particles, allowing larger particles to pass through and resulting in a coarser fines fraction. An air-purged fines outlet prevents any oversized material from bypassing the classifier wheel, while ground material exits the mill for collection downstream.

The internal classifier wheel in fluidized bed jet mills provides exact, reproducible control of particle size distribution. A load cell controls the bed level in the mill, balancing the incoming feed with product discharge. As a result, internal circulation can be up to 20 times that of the mill throughput.

While the performance of a fluidized bed jet mill is sufficient for many applications, there are some drawbacks that make that technology less than ideal for some materials. For example, a residual quantity of material remains in the mill following each run, which is undesirable with materials that are hazardous, toxic, pyrophoric or of very high value. Additionally, very low-density materials cannot "settle" easily in the upward flow of gas in a fluidized bed jet mill and therefore cannot be processed as efficiently as high-density materials.

Figure 2. Operation of the high-density bed jet mill.

Optimized Grinding and Throughput

The new continuous high-density bed jet mill was designed to overcome all of these limitations. The mill features an operating principle similar to that of a spiral jet mill. The feed material is conveyed into the high-density bed through an injector, while the grinding gas enters the mill periphery, accelerating the particles in the bed and reducing particle size through particle-to-particle impact (see Figure 2).

Unlike the spiral jet mill, the high-density bed jet mill features an integrated dynamic air classifier that provides exact and reproducible particle size control, similar to the classifier found in the fluidized bed jet mill. However, because of the high concentration of material in the high-density bed, efficiency can be higher than in fluidized bed jet mills, especially when processing low-density materials. Additionally, minimal residual material remains in the mill after a run, resulting in less waste, less storage, safer handling and reduced downtime for cleaning. The mill also features a compact design that requires less floor space, and smaller mill sizes are available that can be easily installed in glovebox or downflow booth.

The high-density bed jet mill provides value-added processing through high product quality, finer particle size distributions, steeper particle size distributions and reproducible results. Compared to a conventional spiral jet mill, the high-density bed design provides fineness independent of product loading, which allows for higher feed rates and a higher capacity and/or reduced specific energy. Compared to a fluidized bed jet mill, the new mill offers more efficient processing of low-density materials, as well as less risk of contamination from residual materials.

With the new jet mill, companies can achieve both a fine particle size and high-throughput grinding.

For more information about the high-density bed jet mill, contact Netzsch Fine Particle Technology, 125 Pickering Way, Exton, PA 19341; (610) 363-8010; fax (610) 280-1299; e-mail grinding@netzschusa.com; or visit http://www.netzchusa.com. NETZSCH-CONDUX Maltechnik GmbH can be reached at (49) 6181-506-01.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

September 2014 Issue Highlights

Our September 2014 issue is now available!

Posted: December 15, 2014

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!