Decorating with Lasers

The new LMMs are available in a wide range of colors.
For years, laser marking has been widely used in many industries to decorate and identify metals, plastics and other materials, but only recently has it been tested on glass and ceramic materials. Historically, hand painting, inkjet printing and screen printing, as well as heat transfer and water-release ceramic decals, have been the most efficient methods of putting high-quality decorations and images on glass and ceramic surfaces. However, glass and ceramic decorators have been actively investigating other methods that will print high-speed images in any color with simple, quick and low-cost curing. Today, with the advances in marking technology, lasers are rapidly becoming the method of choice for marking and decorating products such as glassware, tableware, sanitaryware and tiles.

Developing Laser Inks and Coatings

The timing of the advances in laser marking technology is crucial to the glass and ceramic industries, as concerns about the toxicity of the solvents and heavy metal pigments used to produce the most vivid colors used in these processes have resulted in increasing regulations in North America and Europe. Additionally, increased competition between ceramic manufacturers and decorators has heightened the urgency to find faster, more efficient methods of marking and decorating.

Conventional decorating methods use a variety of solvents to assist in applying the decorative ink materials. These solvents control the viscosity and rheology of the wet inks and keep them in liquid form during processing. The curing process evaporates the solvent, leaving a stable film adhered to the surface. Heat, an important part of the curing process, accelerates the reaction and increases the adhesion of the ink film to the glass or ceramic substrate.

Aside from visual appearance, adhesion is probably the most important property demanded of a decorative coating on a glass or ceramic surface—and it can also be the most difficult property to achieve. TherMark Corp., headquartered in Los Angeles, Calif., in cooperation with CERAM Research Ltd. and Keele University’s Postgraduate Training Partnership Scheme, both located in the UK, has been working on the development of laser-applied organometallic coatings for decorating tableware. Using new analytical tools to determine what fundamental forces govern the bonding of organometallic and inorganic materials, researchers in these organizations are developing new laser-applied materials to meet both the visual and adhesion demands of the glass and ceramic industry.

The new laser marking materials (LMMs)* being developed through this research are available in liquid form, as a dry transfer tape or label product, and as a dry powder for electrostatic deposition. The liquid LMMs are applied to the substrate surface, dried and then fused to the substrate using laser energy. The laser is operated in a continuous wave mode so that the laser energy is absorbed by the marking material and converted to heat, causing it to permanently adhere to the substrate surface. The laser accomplishes in seconds what would normally require hours in a conventional oven or kiln and consumes only a small fraction of the total energy. Drying the LMM prevents the pigmented material from migrating along the surface of the substrate due to the rapid evaporation of the water-based solution during the laser firing. Finally, the remaining LMM can be brushed or vacuumed off the surface or washed off with a water spray. The liquid materials can be applied using an industrial spray gun, airbrush, brush, roller, pad printer, inkjet printer or screen printing device. The entire process can be automated using standard, off-the-shelf industrial application and cleaning components.

The dry transfer tape or label LMMs consist of a marking material coated onto a backing such as paper or a plastic film. The coating is slightly self-adhesive and is placed in contact with the substrate surface. When laser energy is passed over the tape, the LMM is transferred and permanently bonded to the substrate. Marking on porous ceramic substrates is an ideal application for these dry transfer tape products because the tapes keep the marking material from soaking into the pores of the ceramic surface. This results in increased contrast by keeping the surrounding area clean, without the overspray associated with liquid LMMs, and also eliminates the need to remove any unfired marking material. This type of LMM is especially useful for small production lots because it’s much quicker than liquid LMMs and doesn’t require preparation or cleaning of industrial spraying equipment.

Although the LMMs can be used with most commercially available CO2 and Nd:YAG laser marking systems, a solid-state, diode-pumped fiber laser offers the most durability and flexibility for industrial marking and decoration due to its simplified design and lack of critical optical alignments. Using fiber-delivered laser energy means that only the beam steering head has to be mounted near the product, greatly simplifying the installation of the laser marking equipment in the industrial environment. Laser marking systems allow the decorator to change the image as needed to perform personalized decorations or to serialize individual items.

Sanitaryware manufacturers are using the dry transfer tape LMMs to brand and decorate their products.

Applying the New Technology

The marks made with LMMs withstand high-temperature heat treatment, making them useful for identifying tile bodies, electrical insulators or other ceramic products before glazing. Preliminary tests show that the marks survive temperatures up to 1200?C. Several prominent manufacturers in the sanitaryware industry are currently using the dry transfer tape LMMs for branding and decorating their products, which allows faster turnaround for customized or personalized products and reduces inventory requirements.

Post-fire marks can be made on the back of floor tiles after the glaze has been fired onto the front side of the tile, allowing the manufacturer to apply a glaze and mark a color and/or customer specific code on the reverse side of the tile. Marking tiles in this way eliminates the need for stick-on labels, facilitates manufacturing and distribution, and also serves to better control inventory at the retail level.

Post-fire marking is also currently being used by a major manufacturer of catalytic converters for automobiles to provide permanent product identification and production information markings on the surface of the ceramic cores. The LMM tape is contained in a cassette similar to a typewriter ribbon. The individual ceramic cores are brought into contact with the LMM tape by a robotic handling system, and a message is sent to the laser marking system to write the specific product identification and production information on the product. The robot then removes the ceramic core from the tape surface, the tape advances, and the system is ready for the next part to be presented.

Post-fire marks on items such as this catalytic converter provide permanent product identification.

The Wave of the Future

The LMMs provide a number of advantages compared to conventional decorating materials, including no heavy metal pigments, lower energy consumption and faster curing speeds. They are lead-free, cadmium-free and water-based for quick and easy cleanup. Additionally, they are available in a wide range of colors and feature excellent chemical and abrasion resistance. They have been successfully tested in the industrial environment for caustic cleaning processes, hydrochloric acid dip, sulfuric acid dip, nitric acid dip, heat treatment and the Taber Abrasion Test according to ASTM D 3389, and they are currently being tested for dishwasher durability, weathering and survival in natural acids.

As ceramic and glass manufacturers and decorators seek to make their processes more efficient and environmentally friendly, new decorating and marking techniques will be needed that meet these demands. The new laser marking materials, with their enhanced application speed and performance, will undoubtedly play an important role in this new era.

For More Information

For more information about the new laser marking materials, contact TherMark Corp., 5336 Vincent Ave., Los Angeles, CA 90041; (323) 255-4070; fax (323) 255-3489; or visit http://www.thermark.com.

*supplied under the tradename TherMark™

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!