Sacmi Whiteware: Resin Mold Treatments

Sanitaryware high-pressure casting molds, whether micro- or macroporous, have a working life of some tens of thousands of castings. Two factors determine the extent of that working life -- mechanical stress and clogging of the porous cavities. Until now, there has been no definitive solution for cavity clogging. To resolve this problem and thus make molds last longer, Sacmi Whiteware has patented Everes, a regeneration technique that goes beyond simple cleaning and fully restores original mold performance. Additionally, Loprem is an exclusive production line treatment. Plaster molds used in low-pressure casting have two drawbacks -- long reset times (just 1-2 castings per day) and a limited working life (only about 100 castings). Resin molds could be used to resolve these problems, but only at higher costs and with greater casting pressures. Loprem provides a solution for those aiming at both medium-high complex piece output and cost containment. An innovative technology that allows resin molds to be used with capillary-effect low pressure, Loprem molds provide all the advantages of resin while eliminating its disadvantages.

For more information, visit http://www.sacmi.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!