Corning's HPFS Glass Material Being Tested in Space by NASA

Corning Incorporated recently announced that its HPFS(R) fused silica glass material is being studied by NASA as part of the Materials International Space Station Experiment (MISSE). The project aims to investigate the stability and durability of a variety of materials that are planned for future space applications. Corning has a long history of providing HPFS fused silica glass material to NASA. The company has provided the window glass for every manned space launch of NASA, as well as all of the glass for the space station. The experiment will determine the long-term effects a space environment has on various materials, including Corning's HPFS fused silica glass material. The HPFS and samples of other materials were delivered to the International Space Station (ISS) by the space shuttle Discovery.

More information is available at http://www.hpfs.corning.com or http://www.tropel.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!