The Argonne National Laboratory (ANL) Glass Furnace Model (GFM) was recently selected as one of the 100 most technologically significant products introduced into the marketplace over the past year.

The Argonne National Laboratory (ANL) Glass Furnace Model (GFM) was recently selected by the independent judging panel and editors of R&D Magazine as one of the 100 most technologically significant products introduced into the marketplace over the past year. The GFM software was developed to provide the glass industry with an advanced, state-of-the-art computational fluid dynamics (CFD) software package that could be used as a tool to seek ways to improve productivity and product quality, and reduce furnace energy use and emissions. It generates a computer simulation that allows engineers to "visualize" critical heat transfer, flow and reaction patterns within the interior of a glass furnace, thus helping users to identify sub-optimal performance, both locally and globally. The furnace simulation is used to conduct extensive experiments on the computer by varying key operating and design parameters to determine their impact on overall furnace performance parameters, such as energy use and glass quality indices. By using the GFM code, engineers can conduct extensive computer-based experimental investigations of furnace performance that could not be done on the operating furnace.

ANL is initially offering the GFM on a no-fee trial basis to introduce the code to, and promote its use by, the glass industry. At the conclusion of the no-cost trial-use period, users will be asked to pay a nominal one-time fee to continue using the code. A license can be obtained through the ANL software shop at http://www.softwareshop.anl.gov. For more information, call (630)-252-6518 or e-mail bgolchert@anl.gov.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!