New dispersants are being developed to overcome the recent cost and supply challenges with conventional polyacrylate formulations.



Polyacrylate (PAA) dispersants have been widely used by clay suppliers and ceramic manufacturers to deflocculate clay suspensions and disperse pigments in glazes. These chemicals neutralize surface charges on colloidal particles and disperse the formulation so that a high-solids, low-viscosity slurry or glaze is achieved. Over time, PAAs have replaced more conventional chemistries like silicates and phosphates as deflocculating agents, as many ceramic manufacturers found that PAAs were easier to use and provided better stability.

However, several challenges have recently begun to threaten the availability of these valuable materials. The cost of acrylic acid, the key raw material in the manufacture of polyacrylates, has continued to increase and remains well above historic average price levels. Manufacturers of PAA dispersants also consume raw materials derived from petroleum, natural gas and other commodities that are increasing dramatically in cost, along with the costs of labor, energy and regulatory compliance. Additionally, operational issues have produced "feedstock shortages" for the acrylic monomer producers, which, in turn, have resulted in limited availability of these monomers to PAA manufacturers. And high global demand, driven primarily by China, as well as a lack of investment in additional new capacity, have contributed to the acrylic monomer supply problems. As a result, some ceramic manufacturers are now finding conventional PAA dispersants to be cost-prohibitive, and others are unable to buy PAA dispersants regardless of price.

Fortunately, PAA suppliers are stepping up to the plate and are developing alternatives. Two of the most recent innovations-a non-acrylic acid-based PAA and new blends to replace PAA-are showing particular promise for ceramic applications.

Figure 1. A comparision of the deflocculation curve in a ceramic tile body using a standard PAA (COLLOID 211) and the new non-acrylic acid based PAA (COLLOID 148).

Cost and Performance Benefits

The non-acrylic acid-based PAA, COLLOID 148, was specifically developed to replace a standard PAA dispersant, COLLOID 211. The new dispersant is the same molecular weight and concentration as the previous material, and many ceramic manufacturers who have used the new material have found it to be a direct, equal-dose replacement. Because it does not contain acrylic acid, the new dispersant is readily available at a cost similar to previous acrylic acid-based dispersants.

Figure 1 compares the deflocculation curve in a high-solids, clay-based ceramic tile body using the standard PAA and the new non-acrylic acid based PAA. As can be seen from the data, both additives produce virtually equivalent viscosity at equal dose levels.

For manufacturers that require some PAA for stability, new chemical blends can be used to reduce the amount of PAA required to achieve the same effect. Suppliers have found that using combinations of PAA and other conventional dispersing agents in synergistic ratios can replace PAA at a cost that is equal to or lower than the original treatment. Like COLLOID 148, these proprietary new blends are successfully being used in tile and other clay slurry applications.

Figure 2 illustrates the performance of two of these blends compared to COLLOID 211. As can be seen in the figure, although an increased dosage of the blends is required, a similar deflocculation effect is achieved.

Figure 2. A comparison of the deflocculation curve in a ceramic tile body using a standard PAA (COLLOID 211) and two proprietary polymer blends (TC 9010 and TC G5LE).

Continued Developments

Global production of ceramic products is on the rise, particularly in Asia, and the challenges of high labor, energy and regulatory costs are not likely to disappear any time soon. As a result, PAA dispersants that were once low-cost and readily available are now becoming increasingly expensive and difficult to obtain. Ceramic manufacturers are being forced to choose between buying less of these chemicals than desired at a higher price, or seeking replacements.

Fortunately, some alternatives are now available that offer comparable or even improved performance at a cost equal to or lower than conventional PAAs, and additional developments are under way. By working closely with chemical suppliers, ceramic manufacturers can avoid the PAA supply and pricing issues and find new solutions that give them a competitive edge.

Editor's note: All of the new dispersants and blends described in this article are supplied by Kemira Chemicals, Inc.

For more information about the new dispersants, contact Kemira Chemicals, Inc. at 245 Town Park Dr., Ste. 200, Kennesaw, GA 30144; (800) 347-1542; fax (770) 436-3432; e-mail front-desk@kemira.com ; or visit http://www.kemira.com .

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

September 2014 Issue Highlights

Our September 2014 issue is now available!

Posted: December 15, 2014

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!