Thermal Ceramics: High Alumina Castables

Thermal Ceramics' Kao-Tab® castable line, based on chemically and thermally stable tabular alumina aggregate, has very low levels of alkali and titania impurities, as well as very small amounts of silica. This makes them very resistant to reducing atmospheres and also produces high hot strengths. The company offers four castables in the high alumina castable family: Kao-Tab 95 and Kao-Tab 95 Gun 95% alumina castables designed for casting and gunning, respectively; Kao-Tab SR, an 88% alumina castable designed for placement by gunning or hand ramming; and Kao-Tab HDHS-98, a very high purity, 98% alumina castable with high hot strengths, used for hydrogen atmospheres in the chemical processing industry or high-temperature applications in the iron and steel, cement, and copper industries. For additional information, call (706) 796-4313, fax (706) 560-5841, e-mail wevans@thermalceramics.com or visit http://www.thermalceramics.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!