Alfred's Miller Wins International Research Award (posted 12/11/07)

Michelene E. Miller, who is working on her Ph.D. at the Inamori School of Engineering at Alfred University, is this year’s recipient of the 2007 Excellence in X-Ray Diffraction (XRD) Scholarship award from Bruker AXS. The $6000 scholarship award was announced during the recent fall meeting of the Materials Research Society.

Bruker presents the scholarship annually to graduate students who are doing the most unique research in the field of materials research. Miller, who is advised by Scott T. Misture, Ph.D., professor of Materials Science, submitted a paper entitled “Novel Processing of Microporous Glass-Ceramics for Gas Separation.”

“Using high-temperature X-ray diffraction, we determined that nickel-doped cordierite glass-ceramics are candidates for application as permeability-controlled microporous membranes to separate out carbon dioxide and hydrogen gases in fossil fuel power plants, both reducing greenhouse gas emissions and generating hydrogen,” said Miller.

Misture’s group studies the dynamic behavior of oxide ceramics and glasses related to energy conversion devices. Projects generally rely on detailed in-situ characterization using X-rays and neutrons to understand the relationships between structure and properties. Their recent work has focused on the effects of atmosphere and humidity on structure, phase stability and conductivity at high temperature. Funded by the National Science Foundation, the U.S. Department of Energy, the U.S. Environmental Protection Agency and other agencies, their current research focuses on materials for solid oxide fuel cells and hydrogen production.

Runner-up for the award was Qian Zhang, a Ph.D. student at the University of Montreal. The scholarship winner and runner-up were selected by an independent panel of judges that included Tom Blanton, Ph.D., from Eastman Kodak; Jim Kaduk, Ph.D., from Innovene and current board chairman of the International Centre for Diffraction Data; Pam Whitfield, Ph.D., from National Research Council Canada; Jim Britten, Ph.D., from McMaster University; and Nattamai Bhuvanesh, Ph.D., Department of Chemistry at Texas A&M University.

“We are quite pleased again this year to provide a Bruker XRD scholarship to another extraordinary student,” said Uwe Preckwinkel, Bruker AXS XRD sales and marketing manager.

“Both Bruker AXS and the judges are most impressed by the quality of the XRD experiments all these future X-ray scientists have performed, and the valuable scientific results they have obtained,” said Frank Burgaezy, Ph.D., executive vice president of Bruker AXS in charge of the company’s global XRD and XRF business.

For more information, visit www.alfred.edu.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!