NexTech and Plug Power Complete 2-KW Fuel Cell Project (posted 7/2/08)

Joint activities included market research, fuel cell stack development and testing, system design, and prototype construction.

NexTech Materials, Ltd. and Plug Power Inc. have concluded their two-year collaboration to develop a solid oxide fuel cell (SOFC) power system. The two companies completed a number of joint activities, including market research, fuel cell stack development and testing, system design, and prototype construction at both NexTech and Plug Power facilities.

“Completion of this important project positions NexTech to move forward in both the commercial and military power markets,” said Bill Dawson, president/chief executive officer of NexTech. “NexTech has developed and demonstrated its planar 2-kW level SOFC stack, as well as internal reforming of methane.” NexTech plans to work with system integrators to develop products for remote power, transportation auxiliary power units (APUs), combined heat and power, and large commercial stationary applications using its sulfur-tolerant, high-performance stack technology.

Plug Power determined the system requirements and the process design, and developed the balance of plant for the unit, which operated on both hydrogen and methane. According to William D. Ernst, Ph.D., vice president and chief scientist for Plug Power, “This project provided an excellent opportunity for us to evaluate the potential for the innovative SOFC technology developed by NexTech to satisfy the market requirements for continuous power systems.”

SOFC systems offer potential performance advantages for power applications where the use of commonly available fuels is required. They have been demonstrated to produce power at the highest efficiency of any fuel cell and can operate on natural gas and propane. Work is underway to utilize coal gas, diesel, gasoline and kerosene fuels in these environmentally friendly fuel cell systems.

Partners in this project included the Ohio Department of Development, which provided essential seed funding through the Third Frontier Program, and Case Western University, which will develop testing methodologies to help minimize development cycle time through work at the Wright Fuel Cell Group.

For additional information, visit www.nextechmaterials.com or www.plugpower.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!