KaMin Announces Price Increases (posted 6/11/08)

KaMin LLC, formerly the Kaolin Business Unit of J.M. Huber Corp., recently announced that, due to soaring inland and ocean freight rates combined with escalating fuel surcharges, price increases will be implemented on all export-delivered kaolin clay pricing to industrial specialties markets effective July 1, 2008. “We have continued to absorb the punishing effects of general rate increases and fuel surcharges implemented by ocean, truck and rail providers,” said Tom Anderskow, vice president of Sales and Marketing. “These price increases are necessary to allow KaMin LLC to provide the superior service our international customers have come to expect.”

For more information, visit www.kaminllc.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 February

You won't want to miss this issue, which includes our annual R&D Lab Equipment and Instrumentation Directory!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!