NREL Solar Cell Sets World Efficiency Record at 40.8% (posted 8/29/08)

Scientists at the U.S. Department of Energy’s (DOE) National Renewable Energy Laboratory (NREL) have set a world record in solar cell efficiency with a photovoltaic device that converts 40.8% of the light that hits it into electricity. This is the highest confirmed efficiency of any photovoltaic device to date.

The inverted metamorphic triple-junction solar cell was designed, fabricated and independently measured at NREL. The 40.8% efficiency was measured under concentrated light of 326 suns. (One sun is about the amount of light that typically hits Earth on a sunny day.) The new cell is a natural candidate for the space satellite market and for terrestrial concentrated photovoltaic arrays, which use lenses or mirrors to focus sunlight onto the solar cells.

The new solar cell differs significantly from the previous record holder, which was also based on a NREL design. Instead of using a germanium wafer as the bottom junction of the device, the new design uses compositions of gallium indium phosphide and gallium indium arsenide to split the solar spectrum into three equal parts that are absorbed by each of the cell’s three junctions for higher potential efficiencies. This is accomplished by growing the solar cell on a gallium arsenide wafer, flipping it over, and then removing the wafer. The resulting device is extremely thin and light, and it represents a new class of solar cells with advantages in performance, design, operation and cost.

NREL’s Mark Wanlass invented the original inverted cell, which recently won a R&D 100 award. His design was modified by a team led by John Geisz that further optimized the junction energies by making the middle junction metamorphic as well as the bottom junction. Metamorphic junctions are lattice mismatched (i.e., their atoms don’t line up). The material properties of the mismatched semiconductors allow for greater potential conversion of sunlight.

NREL is the DOE’s primary national laboratory for renewable energy and energy efficiency research and development. NREL is operated for the DOE by Midwest Research Institute and Battelle. For more information, call (303) 275-4090 or visit www.nrel.gov.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 February

You won't want to miss this issue, which includes our annual R&D Lab Equipment and Instrumentation Directory!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!