Demand for metal injection molded parts will grow 14.0% annually through 2014, well ahead of plastics injection molding, according to a new technical market research report, “Metal and Ceramic Injection Molding (AVM049B),” from BCC Research. The global market for metal injection molding (MIM) will be worth $984.9 million in 2009, and is expected to increase to $1.9 billion in 2014. Demand for ceramic injection molded parts will grow at an even faster rate, 15.2% annually.

“Powder injection molding (PIM) is booming on a global basis because of its ability to either create unique new products or replace older technologies at significant savings,” according to the introduction to the 242-page analysis. “The process allows design of the very complex, net shapes that are made via plastic injection molding, but in materials-metals and ceramics-that have properties far in excess of plastic.”

The industry must still overcome several challenges, including lack of awareness of the process among design engineers, a weak reputation in some quarters for repeatable dimensional control, high materials prices and lack of standardization, states the report. Aiding development is the substantial move to improve processing technology and materials.

The global ceramic injection molding (CIM) market is expected to be worth $394.5 million in 2009 and $801.0 million in 2014, a compound annual growth rate (CAGR) of 15.2%. Broken down by geographic region, North America captures the largest share of the market and is expected to generate $276.5 million in 2009 and $512.6 million in 2014, for a CAGR of 13.1%. Europe is the next largest CIM segment of the market, worth an estimated $75.1 million in 2009 and $152.2 million in 2014, a CAGR of 15.2%. The third-largest market CIM segment is Asia, which is expected to generate $39.5 million in 2009. This should increase at a CAGR of 24.9% to reach $120.2 million in 2014.

For more information, call (866) 285-7215, e-mail editor@bccresearch.com or visit www.bccresearch.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!