Both instruments in the new line have the ability to operate within a wide range of temperature (-260 to 500°C) and pressure (vacuum to 200 bar).

Setaram recently announced the latest addition to its Hy-Energy product line, the PCTPro-E&E (energy and environment). This completely automated Sievert gas sorption instrument is capable of using multiple gases to characterize today’s most promising materials.

Two versions of the PCTPro are available: PCTPro-2000 and PCTPro-E&E. Both of these instruments have the ability to operate within a wide range of temperature (-260 to 500°C) and pressure (vacuum to 200 bar).

The PCTPro-E&E is ideally suited for the study of carbon capture and sequestration (CCS) materials and methane sorption onto geological substrates. Applications include gas-reaction compounds and high-surface-area adsorbents, including carbon materials (nanopowders, films, fibers, nanotubes); adsorbents for CO2 storage and separation; activated alumina (gas and liquid purification); molecular sieves (zeolites, MOFs, etc. for gas separation and vapor removal); and methane adsorption on substrates.

The PCTPro-2000 is designed for the characterization of hydrogen sorption properties of a wide range of materials, including gas-reaction compounds and high-surface-area adsorbents such as hydrogen storage materials (metal hydrides, alanates, amides, MOFs) and carbon materials (nanopowders, films, fibers, nanotubes).

For more information, call (510) 793-3345, fax (510) 402-4705 or visit www.setaram.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 February

You won't want to miss this issue, which includes our annual R&D Lab Equipment and Instrumentation Directory!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!