The windshields and side cockpit windows for the Citation Columbus are expected to be similar to those that PPG supplies for other business jets.

PPG Industries’ Aerospace Transparencies business has been awarded a contract by Cessna Aircraft Co. to develop and produce all-glass heated cockpit windows for the new Citation Columbus business jet. Terms were not disclosed. PPG will supply shipsets for Cessna’s production, as well as spares, according to Ann Wommack, PPG senior account manager.

The windshields and side cockpit windows for the Citation Columbus business jet are expected to be similar to those that PPG supplies for Cessna’s Citation VII, Citation X, Citation Excel, Citation Sovereign and Citation CJ4 business jets. “PPG has a long history supplying cockpit windows to Cessna, and we are pleased to be able to work with them on this exciting new platform,” said Wommack.

The cockpit windows for the Columbus jet will have three plies of PPG’s Herculite II glass, which is chemically tempered for high strength at light weight, and the Nesatron heating system, according to Wommack. The windshields will also have Surface Seal hydrophobic coating for rain clearing and an antistatic coating to redirect static discharge, enhancing the life of the Surface Seal coating. Using Surface Seal coating on windshields enables Cessna to pursue certification without wipers on its planes, she said.

The transparencies will be produced at PPG’s Huntsville, Ala., aircraft products plant. The Citation Columbus is expected to gain full certification in 2013 and enter service in 2014. Visit www.ppg.com for more information.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!