ENrG Inc. recently announced that it has entered into a licensing agreement with Corning Inc. that enables ENrG to produce thin ceramic membranes with unique properties for solid oxide fuel cells (SOFCs). The advanced technology will allow for the production of electrolyte-supported fuel cells with extremely thin profiles, excellent thermal cycle performance and high durability. Since SOFC fuel cells undergo repeated thermal cycling, the thin membranes combine the strength and high energy performance best-suited for fuel cell stack designs.

Through a New York State Energy Research and Development Authority (NYSERDA)-funded initiative, “Fabrication of Tri-Layer Cells Based on ≤ 50 micron Zirconia Tape for the Solid Oxide Fuel Cell Market,” ENrG will complete the infrastructure to begin fabricating thin fuel cell devices. ENrG has several years of experience in handling and printing on thin electrolytes, and this initiative is an extension of ENrG’s experience in this area.

In addition, NYSERDA has awarded ENrG a contract to support market entry to reach fuel cell companies in Europe, Canada, Japan and the U.S. in an effort to expand the marketplace for this technology. The updating of ENrG’s website, combined with new literature, sample presentations and a presence at major energy shows, will advance the company’s products to end-users.

“We are pleased to extend our partnership with ENrG as we work toward the goal of commercializing fuel cell components for the fuel cell industry,” said Francis J. Murray, president and chief executive officer of NYSERDA. “A future with alternative, clean energy solutions is a priority for NYSERDA, and our agreement with ENrG Inc. will continue New York State’s commitment to reduce air pollution and advance environmentally safe, fuel-efficient technologies.”

For additional information, visit www.enrg-inc.com, www.corning.com or www.nyserda.org.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!