Ceramic Industry News

KEMET to Manufacture Standard DC Film Capacitors in Mexico (posted 11/18/09)

November 18, 2009
/ Print / Reprints /
ShareMore
/ Text Size+

KEMET Corp. recently announced that it is preparing its Monterrey, Mexico, Guadalupe Campus to manufacture standard DC film capacitors. “This is the first of many steps that we will be taking to restructure this business group to lower our manufacturing cost through moving production to lower-cost centers and leaning out any waste within production,” said Per Loof, CEO. “There are great opportunities for our Film and Electrolytic Business Group in the Americas. We are seeing real growth in many of the markets for which these products are used, such as alternative energy. Additionally, this move positions us closer to the growing Americas customer markets, allowing us to work in partnership on the design-in phase of projects that is so important with these technologies.”

This new manufacturing capability in North America is in addition to the U.S. Department of Energy grant the company previously announced regarding new power film and electrolytic manufacturing capabilities at its Simpsonville, S.C., campus. It is expected that equipment will be transferred to Monterrey over the December holiday period, with production beginning 90-120 days later.

“As a result of the utilization of lean manufacturing techniques, the Ceramic Business Group has been able to reduce the amount of required floor space to support Ceramic operations in the Guadalupe Campus by 50%,” said Kirk Shockley, vice president of the Film and Electrolytic Business Group. “This move will allow the Film and Electrolytic Business Group to support our current and future customers for standard film products in the Americas region through improved logistical responsiveness. Additionally, we will see reduced manufacturing cost through the synergies of producing in a lower-cost environment and sharing infrastructure costs.”

Additional information is available at www.kemet.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!