KILN CONNECTION: Pulse Perfect

Figure 1. Initial pulsing systems often caused somewhat cyclical heating and cooling due to the relatively long high-fire time and sometimes exceedingly long minimum-fire times.

After 35 columns over 10 years with Ceramic Industry, I have covered a lot of territory, ranging from efficiency to temperature uniformity. Along the way, I’ve outlined a range of combustion systems and operational techniques. Kiln technology advancement seems to be more of a step-change than a gradual evolution, and the step improvement that has occurred over the last 15 years has been related to pulse firing and control.

The initial pulsing systems used in this country were generally based on the idea of firing each burner for a fixed amount of time-say 8-12 seconds-and then forcing the burner to low-fire for a variable amount of time. While these types of systems worked adequately, they often caused somewhat cyclical heating and cooling due to the relatively long high-fire time and sometimes exceedingly long minimum-fire times.

The DataPaq curve shown in Figure 1 illustrates the cyclical heating associated with this type of pulsing logic. At the start of the cycle, no pulsing occurred at all because the kiln temperature was above set point. As the kiln approached 350-400°F, pulsing initiated and cyclical heating and cooling occurred in products set close to the burners.

Figure 2. Smoother heating occurs when the high-fire time is kept shorter.

As the system designs evolved, it became obvious that shorter bursts of energy, applied more frequently, would provide a smoother heating characteristic. Additionally, to obtain the best control, particularly near the beginning of the cycle, it was helpful to adjust the burners for the lowest possible minimum firing rate. In this way, almost all of the energy is applied to the kiln process at high fire, ensuring the best possible circulation.

The smoother heating shown in Figure 2 occurred because the high-fire time was much shorter. The burner fired in pulses as short as a half-second, and pulsing occurred regularly every 8-10 seconds. The combination of short periods of input and frequent pulsing allowed for smooth temperature control with all of the benefits of pulse firing, including the minimum use of required excess air, which translates to better efficiency, and reduced NOx formation due to reduced excess air and high-velocity entrainment, which lowers the flame temperature.

As you upgrade your kilns or purchase new kilns, be aware that while pulse firing is the best current combustion solution, the details of the pulsing can make a huge difference in ultimate performance and efficiency.

Any views or opinions expressed in this column are those of the author and do not represent those of Ceramic Industry, its staff, Editorial Advisory Board or BNP Media.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Recent Articles by Ralph Ruark

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!