Corning Filters Selected by Ford of Europe (posted 10/12/09)

Corning Inc. recently announced that Ford of Europe is equipping several models of its European market diesel passenger cars with the Corning® DuraTrap® AT filter. Corning has begun shipping the product to Ford of Europe.

“This is a significant opportunity,” said Thomas R. Hinman, senior vice president of Corning Environmental Technologies. “Ford of Europe is one of the largest diesel car manufacturers in Europe. We are pleased that they have integrated the DuraTrap AT filter into their emissions control systems. Corning’s AT filter technology will help them meet stringent operating conditions and strict regulations.”

The Corning DuraTrap AT filter uses an advanced aluminum titanate composition that delivers enhanced durability, high-filtration efficiency and excellent pressure drop within exhaust after-treatment systems. This filter also uses a monolithic structure that contributes to its durability. The DuraTrap AT filter is being used around the world to help customers meet stringent particulate emissions regulations. It is designed for use in light-, medium-, and heavy-duty diesel vehicles.

Corning diesel filters are used in emission control systems to remove particulate matter (soot) from vehicle exhaust. These wall-flow filters collect soot particles using a cellular ceramic structure with alternating channels open at the inlet and plugged on the outlet of the filter. Periodically the filter is regenerated to consume the soot and clean the filter.

Visit www.corning.com for additional information.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available!

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!