Lowering Fuel Cell Costs

A new sulfur- and coking-tolerant ceramic material could expand applications for SOFCs.

Professor Meilin Liu provides a closer look at the anode side of a laboratory-scale button fuel cell, which includes the new material. Shown (left to right) are Mingfei Liu, Meilin Liu, Kevin Blinn and Lei Yang.


A new ceramic material described in a recent issue of the journal Science could help expand the applications for solid oxide fuel cells (SOFCs). Though the long-term durability of the new mixed ion conductor material must still be proven, its development could address two of the most vexing problems facing SOFCs: tolerance of sulfur in fuels and resistance to carbon build-up known as coking. The new material could also allow SOFCs, which convert fuel to electricity more efficiently than other fuel cells, to operate at lower temperatures, potentially reducing material and fabrication costs.

“The development of this material suggests that we could have a much less expensive solid oxide fuel cell, and that it could be more compact, which would increase the range of potential applications,” said Meilin Liu, a Regent’s professor in the School of Materials Science and Engineering at the Georgia Institute of Technology. “This new material would potentially allow the fuel cells to run with dirty hydrocarbon fuels without the need to clean them and supply water.”

New Material

Like all fuel cells, SOFCs use an electrochemical process to produce electricity by oxidizing a fuel. As the name implies, SOFCs use a ceramic electrolyte, yttria-stabilized zirconia (YSZ). The fuel cell’s anode, which uses a composite consisting of YSZ and nickel, provides excellent catalytic activity for fuel oxidation, good conductivity for collecting current generated, and compatibility with the cell’s electrolyte.

But the material has three significant drawbacks: even small amounts of sulfur in the fuel “poison” the anode to dramatically reduce efficiency; the use of hydrocarbon fuels creates carbon build-up, which clogs the anode; and, because YSZ has limited conductivity at low temperatures, SOFCs must operate at high temperatures. As a result, fuels used in SOFCs, such as natural gas or propane, must be purified to remove sulfur, which increases their cost.

Water in the form of steam must also be supplied to a reformer that converts hydrocarbons to hydrogen and carbon monoxide before being fed to the fuel cells, adding complexity to the overall system and reducing energy efficiency. And the high-temperature operation means that the cells must be fabricated from costly exotic materials, which makes SOFCs too expensive for many applications.

The new material developed at Georgia Tech addresses all three of those anode issues. Referred to as BZCYYb (barium- zirconium-cerium-yttrium-ytterbium oxide), the material tolerates hydrogen sulfide in concentrations as high as 50 ppm, does not accumulate carbon and can operate efficiently at temperatures as low as 500°C.

The BZCYYb material could be used in a variety of ways, including as a coating on the traditional Ni-YSZ anode, as a replacement for the YSZ in the anode and as a replacement for the entire YSZ electrolyte system. Liu believes the first two options are more viable.

Commercialization

So far, the new material has provided steady performance for up to 1000 hours of operation in a small laboratory-scale SOFC. To be commercially viable, however, the material will have to be proven in operation for up to five years, the expected lifespan of a commercial SOFC.

“We don’t see any problems ahead for fabrication or other issues that might prevent scale-up,” said Liu. “The material is produced using standard solid-state reactions and is straightforward.”

The researchers don’t yet understand how their new material resists deactivation by sulfur and carbon, but they theorize that it may provide enhanced catalytic activity for oxidizing sulfur and both cracking and reforming hydrocarbons. In addition to its tolerance of sulfur and resistance to coking, the BZCYYb material’s conductivity at lower temperature could also provide a significant advantage for SOFCs.

“If we could reduce operating temperatures to 500 or 600°C, that would allow us to use less-expensive metals as interconnects,” Liu noted. “Getting the temperature down to 300 to 400 degrees could allow the use of much-less-expensive materials in the packaging, which would dramatically reduce the cost of these systems.”

Beyond its use in fuel cells, the material developed by Liu and his team, which also included Lei Yang, Shizhong Wang, Kevin Blinn, Mingfei Liu, Ze Liu and Zhe Cheng, could also be used for fuel reforming to feed other types of fuel cells. Though the technology for SOFCs is currently less mature than that of other types of fuel cells, Liu believes SOFCs will ultimately win out because they don’t require precious metals such as platinum and their efficiency can be higher-as much as 80% with co-generation use of waste heat.

“Solid oxide fuel cells offer high energy efficiency, the potential for direct utilization of all types of fuels, including renewable biofuels, and the possibility of lower costs since they do not use any precious metals,” said Liu. “We are working to reduce the cost of solid oxide fuel cells to make them viable in many new applications, and this new material brings us much closer to doing that.”

This research was supported by the U.S. Department of Energy’s Basic Energy Science Catalysis Science Program under grant DE-FG02-06ER15837. Visit www.gatech.edu for more information. 

Editor’s note: The comments and conclusions in this document are those of the researchers and do not necessarily represent the views of the U.S. Department of Energy.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

Recent Articles by John Toon

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

June 2015 ceramic industry

2015 June

This issue features our first annual Supplier of the Year Awards. Be sure to check it out!
Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!