Corning Launches Slim LCD Glass Substrates

Corning Inc. recently introduced EAGLE XG® Slim, a new line of thin glass substrates. These substrates can allow for lighter-weight portable devices, with glass sizes up to Generation 5 at 0.4 mm thick. Corning plans to add more sizes and thicknesses to the line to support larger applications like LCD TVs.

“As the first to supply commercial volumes of 0.5 mm glass and now 0.4 mm glass, Corning is pleased to apply its technology leadership to help enable the industry’s continued advancement,” said James P. Clappin, president of Corning Display Technologies. “EAGLE XG Slim glass will allow device makers to reduce costs and provide a greener product while creating the sleek, multifunctional devices consumers desire.”

Most panel makers currently begin with 0.5-mm-thick substrates for portable devices, then use a costly thinning process that uses chemicals to reduce the thickness of the glass. Corning’s proprietary fusion process forms thin glass of pristine surface quality, ready to use as-formed. Thin input glass requires no additional panel thinning to achieve weight and thickness targets. Benefits include a lower total cost, a simplified supply chain and reduced energy consumption. In addition, the new substrates will leverage the award-winning EAGLE XG composition, an environmentally friendly glass substrate, making devices even more recyclable.

The EAGLE XG Slim will be produced at the company’s plants in Asia using its worldwide supply chain. Samsung Corning Precision Materials Co., Ltd. will also supply the product line to customers in Korea.

For more information, visit www.corning.com.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!