Ceramic Industry News

Asahi to Sell Glass-Ceramic Substrate

Asahi Glass Co., Ltd. (AGC) has announced it will start sales of a new glass-ceramic substrate that enables high-brightness and high-durability for LED lighting. This new glass-ceramic substrate will expand LED applications in the lighting and illumination sector, including 3-D televisions and automotive lighting, in which high-power output is increasingly in demand. Starting the volume production at a newly built factory in Taiwan, AGC reports that it plans to achieve a market share of 20% or more in the glass-ceramic substrate market for high-output LED lighting, which is expected to grow into a 100 billion yen (about US$1 billion) market by 2020.

LED applications are currently limited primarily to products with extremely small power output, such as liquid crystal display televisions and home interior lighting. In the future, however, the demand trend is expected to shift toward high-output LED applications that require high brightness, such as 3-D televisions, automotive headlights, and other automotive lighting and outdoor lighting and illumination. In addition to high brightness, high durability is also a prerequisite for high-output LED applications, as heat generation becomes greater as the power output increases.

For more information, phone (81) 3-3218-5260 or visit www.agc.co.jp.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

June 2015 ceramic industry

2015 June

This issue features our first annual Supplier of the Year Awards. Be sure to check it out!
Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!