Caroma Chooses Sacmi Plaster Mold Technology

November 17, 2010
/ Print / Reprints /
ShareMore
/ Text Size+

After more than a century, Caroma Dorf has discontinued the use of plaster molds, replacing them with higher performance Sacmi resin molds that can operate at a pressure of 15 bar. Caroma, a member company of GWA Intern. Ltd., has now inaugurated an ALS 150 system at its Sydney plant, which features robotized de-molding and laser-guided vehicle piece transfer.

The technology offers a high automation level of the production cycle, which includes a 90° drying station. In the current configuration, actual piece handling is only required when the supports are loaded on the tunnel kiln cars.

For more information, visit www.sacmi.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

September 2014 Issue Highlights

Our September 2014 issue is now available!

Posted: December 15, 2014

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!