A coating that enables engineers to specify lighter-weight carbon composite materials for harsh environment applications has received the 2010 Plastic Industry Best Technology Application of the Year Award. Zircotec’s plasma-sprayed zirconia-based coating protects composites from the effects of heat and abrasion in tough operating environments, opening up a new stream of materials to designers that offer performance with a weight advantage. The Zircotec coating, ThermoHold® for composites, is being successfully used in F1 this year to allow 650°C exhaust gases to be routed through the car’s carbon fiber diffuser, but is increasingly finding applications in a range of other sectors from aerospace to carbon composite cycle wheels where it is used as a high-performance braking surface.

“Zircotec is delighted to receive the recognition of such an important award,” said Terry Graham, managing director. “We want to increase awareness of the opportunities our coatings offer to the plastics industry, and this is a fantastic way to start engaging with the sector.”

The coating is applied by the firm using a plasma spray process to a thickness of less than 500 microns. Carbon composite components can be coated with ceramic, aluminum, stainless steel and molybdenum to protect against temperature, wear or a combination of the two. Outside of motorsport applications, the coating is planned to be used on an automobile and in a marine application.

For more information, visit www.zircotec.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!