OWENS CORNING: Glass Fiber Reinforcements Guide

This company recently presented a chemical resistance guide for glass fibers at the international trade show for the National Association of Corrosion Engineers. The guide provides information to help end users, engineers and fabricators select glass fiber reinforcements for use in fiberglass-reinforced polymer (FRP) applications used in corrosive environments.

“We talked with specifiers and end users and realized that the corrosion market was missing an important tool,” said Ashish Diwanji, vice president, Innovation, Composite Solutions business. “This guide will help FRP designers balance cost and performance when selecting the best glass fiber to meet their needs.”

The “Glass Fiber Reinforcement Chemical Resistance Guide” contains test results, examples of specifications and information about industry standards for glass fiber compositions used in FRP applications. The results were compiled from tests conducted in the laboratory and knowledge gained in the company’s field experience, and illustrates the effect of various chemicals on different glass fibers. Examples of writing specifications are provided to ensure accuracy and consistency. The company included industry standards for glass fibers used to resist corrosion because selecting the right glass fiber is a key factor in corrosion resistance and can lower the risk of failure.

For more information, visit www.owenscorning.com/composites/aboutAdvantex.asp.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!