Study: Brick Veneer Driest of Exterior Walls Tested

A new study by the NAHB Research Center comparing moisture resistance among typical residential exteriors evaluated brick veneer as the highest in moisture resistance and dryness. As the trend toward lighter, tighter building methods continues to raise moisture concerns, the study aimed to determine how exterior cladding can impact the moisture content of the wooden components in the wall construction. Of the eight wall systems tested-accounting for approximately 90% of the cladding systems used today-brick veneer wall assemblies performed the best overall in controlling moisture.

“The lab report’s findings on brick’s superior moisture resistance are extremely significant,” said J. Gregg Borchelt, president and CEO of the Brick Industry Association (BIA).

The BIA, along with the U.S. Department of Agriculture’s Forest Products Laboratory and the U.S. Department of Housing and Urban Development, funded the study.

“Builders will want to choose brick if they wish to provide their customers the protection of a superior wall system-instead of one that is just ‘good enough,’” Borchelt said.

Modern construction practices to increase comfort and energy efficiency have resulted in tight walls that are highly insulated and sealed against air filtration. When moisture is not sufficiently controlled, risks increase dramatically for mold growth, wood rot and infestation by insects, reduced efficiency of insulation, and corrosion of fasteners. The report attributes the lower moisture content in the wood components to brick’s inherent thermal mass properties, the 1-in. air space in the brick veneer wall and the increased thermal absorption of the test brick’s red color.

Moisture performance values were collected at regular intervals from key components within a pair of wall assemblies constructed with eight different cladding types. Each wall assembly consisted of interior gypsum board and wood studs with fiberglass insulation between the studs, sheathed with either OSB or plywood and clad with brick veneer, vinyl siding, fiber cement, manufactured stone, or stucco. The assemblies were then subjected to ambient weather conditions over a one-year period. A portion of water-resistant barrier was compromised and the wall assembly behind it subjected to a daily water injection over a five-day period to evaluate its ability to dry after a leak.

For more information, visit www.gobrick.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!