Fuel Cells in Operation: A Closer Look

A team of scientists has used a new kind of XPS to examine every feature of a working solid oxide electrochemical cell.

Hendrik Bluhm, Michael Grass, Zahid Hussain and Zhi Liu with the APXPS detection system at beamline 11.0.2. (Photo by Roy Kaltschmidt, Berkeley Lab Public Affairs.)


Measuring a fuel cell's overall performance is relatively easy, but measuring its components individually as they work together is a challenge. That's because one of the best experimental techniques for investigating the details of an electrochemical device while it's operating is X-ray photoelectron spectroscopy (XPS). Traditional XPS works only in a vacuum, while fuel cells need gases under pressure to function.

Now a team of scientists from the University of Maryland, the U.S. Department of Energy's (DOE) Sandia National Laboratories and the DOE's Lawrence Berkeley National Laboratory has used a new kind of XPS, called ambient- pressure XPS (APXPS), to examine every feature of a working solid oxide electrochemical cell. The tests were made while the sample cell operated in an atmosphere of hydrogen and water vapor at one millibar pressure (about one-thousandth atmospheric pressure) and at very high temperatures of up to 750°C (1382°F).

"Our team, led by Bryan Eichhorn of the Department of Chemistry and Biochemistry at the University of Maryland, combined the expertise in fuel cells at U Maryland, the experience of our Sandia Lab colleagues in collecting electrochemical data, and Berkeley Lab's own development of a method for doing X-ray photoelectron spectroscopy in situ," said Zahid Hussain of Berkeley Lab's Advanced Light Source (ALS). "Together we were able to measure the fundamental properties of a solid oxide fuel cell under realistic operating conditions."

Figure 1. In a basic SOFC, the cathode on one side of the electrolyte ionizes oxygen, which flows through the electrolyte to the anode (left), where fuel is oxidized to free electrons. In the model cell built for the APXPS experiment, all the components are on the same side of the electrolyte so they can be reached by the X-ray beam.

How a Solid Oxide Fuel Cell Works

Like a battery, a fuel cell is a device that uses chemical reactions to produce electricity. Unlike a battery, a fuel cell won't run down as long as it's supplied with fuel and oxidant from outside. The main components are two electrodes (an anode and a cathode) separated by an electrolyte.

In a solid oxide fuel cell (SOFC), the cycle begins at the cathode, which ionizes oxygen (usually from air) by adding free electrons. These oxygen ions then flow through the solid oxide electrolyte (from which the SOFC gets its name), which is often yttria-stabilized zirconia. A high temperature is needed to maintain good conduction of oxygen ions through the electrolyte.

In a basic SOFC, as shown in Figure 1, the cathode on one side of the electrolyte ionizes oxygen, which flows through the electrolyte to the anode, where fuel (pure hydrogen gas or a hydrocarbon) is oxidized to free electrons. In the model cell built for the APXPS experiment, all the components are on the same side of the electrolyte so they can be reached by the X-ray beam.

Electrons freed by oxidation form the current in the device's electrical circuit and eventually return to the cathode. Unused fuel or other compounds, plus water formed from the positive hydrogen ions and negative oxygen ions, exits the fuel cell.

For the APXPS experiment, the University of Maryland collaborators built a model fuel cell that combined the essential elements of an SOFC in a special miniaturized design of less than 2 mm in length. Except for the electrolyte of yttria-stabilized zirconia, which formed the base of the device, the various components were thin films measuring from 30 nanometers (billionths of a meter) up to 300 nanometers thick.

"We designed and fabricated solid oxide electrochemical cells that provided precise dimensional control of all the components, while providing full optical access to the entire cell from anode to cathode," said Eichhorn.

Instead of stacking the components as in a real fuel cell, the sample's arrangement was a planar design that placed all the components on the same side of the electrolyte, so the X-ray beam from the ALS could reach them. This allowed direct measurement of local chemical states and electric potentials at surfaces and interfaces during the cell's operation.

Figure 2. Using an electrostatic lens, the APXPS detector collects photoelectrons emitted from the surface of the sample by the X-ray beam. Chemical states (green circles) and electric potentials (red squares) are measured locally. The greatest activity was measured where the electrode (green) met the electrolyte (blue).

Introducing APXPS

Photoemission occurs when light ejects electrons from a material. By collecting the emitted electrons and analyzing their energies and trajectories, photoelectron spectroscopy establishes exactly what elements are in the material and their chemical and electronic states within narrow regions. At the ALS, intense X-ray light is used to explore what happens at or near the surface of materials: the only photoelectrons that can escape are from atoms near the surface.

The APXPS system begins by shining the X-ray beam on the sample fuel cell inside a chamber at the ambient pressure of the gas needed for it to operate (see Figure 2). The emitted electrons then travel through chambers pumped to lower pressure, finally entering the high-vacuum chamber of the detector. By itself, this arrangement would lose emitted electrons at every stage because of their spreading trajectories, leaving a signal too weak to be useful. So Berkeley Lab researchers developed a system of "lenses"-not made of glass but of electric fields-to capture and refocus the emitted electrons at each stage, preventing excessive loss.

"This is what allows us to find out what's happening within small regions on the surface of a sample in the presence of a gas," said Hendrik Bluhm of Berkeley Lab's Chemical Sciences Division and one of the inventors of APXPS. "Using the APXPS instruments at the ALS's molecular environmental science beamline, 11.0.2., and the chemical and materials science beamline, 9.3.2, we can spatially correlate the catalytic activity with the electrical potentials across the different components of the model fuel cells."

"At first, we weren't sure we could use this technique with an operating fuel cell, because we had to bring it to 750°C, an extreme temperature for such ambient pressure experiments," said Zhi Liu of the ALS. "Few people have done it before. Now we're able to perform this kind of analysis routinely."

"What you need to know to improve any kind of fuel cell is where the inefficiencies are, places where energy is being lost compared to what theoretically should be possible," added Michael Grass of the ALS. "By scanning across the surface of the cell while it was operating, we could directly measure both the inefficiencies and the chemical states associated with them."

Researchers used an APXPS system to study the electrochemical properties of a model fuel cell operating at extreme heat.

Studying Electrochemistry in Action

With their model SOFC, the Maryland-Sandia-Berkeley Lab team saw details never before seen in an operating fuel cell. Where an overall measurement gave only the fuel cell's total losses in potential energy, the APXPS measurements found the local potential losses associated with the interfaces of electrode and electrolyte, as well as with charge transport within the ceria electrode. The sum of the losses was equal to the cell's total loss, or inefficiency.

"The in situ XPS experiments at 750°C allowed us to pinpoint the electroactive regions, measure length scales of electron transport through mixed ionic-electronic conductors, and map out potential losses across the entire cell," said Eichhorn. "Others have suggested similar experiments in the past, but it was the remarkable facilities and scientific expertise at the ALS that facilitated these challenging measurements for the first time."

APXPS can provide this kind of fundamental information to SOFC designers, information not available using any other technique. New fuel cell designs are already taking advantage of this new way to study fuel cells in operation.

The researchers reported their results in the November 2010 issue of Nature Materials.Berkeley Lab is a U.S. Department of Energy national laboratory located in Berkeley, Calif. It conducts unclassified scientific research for the DOE's Office of Science and is managed by the University of California. For additional information, visit www.lbl.gov.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!