Georgia Tech Awards Project to Harper International

Harper International announced it has been awarded a project by the Georgia Institute of Technology for the production of a university-scale carbon fiber (CF) thermal processing system. Georgia Tech has been provided Defense Advanced Research Projects Agency (DARPA) funding in the area of carbon fibers and partnered with Harper to develop a customized process system for its research purposes.

Georgia Tech required an especially distinctive configuration in the line to accommodate fractional tow sizes in the range of less than 100 filaments. This condition pushes the boundaries for typical carbon fiber processing, as traditional commercial CF lines handle tow sizes of 3K, and rarely down to 1K. Harper’s design team created a proprietary solution to this challenge, enabling researchers to achieve their goals of processing material more quickly and using less expensive additives.

“Harper’s thermal processing systems will be used in our advanced materials research at Georgia Tech,” said Satish Kumar, Ph.D., professor at the School of Materials Science and Engineering. “Solving tough problems with real-world solutions is part of what we do at Tech. We are always interested in finding creative, technologically-focused partners to assist with our research.”

Carbon fibers, including those containing carbon nanotubes (CNTs), are a prime area of focus in advanced materials research due to their increased strength, flexibility, and unique electrical properties. CNTs can be used in applications across almost all fields of science, engineering, and technology, and help expand the realm of nanotechnology through their use in the control of other nanoscale structures.

For additional details, visit www.harperintl.com or www.gatech.edu.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 February

You won't want to miss this issue, which includes our annual R&D Lab Equipment and Instrumentation Directory!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!