Lucifer Furnaces Builds Fiber-Lined Oven for Lincoln Electric

Lucifer Furnaces recently announced it has delivered a large fiber-lined forced-air recirculating oven to The Lincoln Electric Co., Cleveland, Ohio. With chamber dimensions of 24 x 24 x 36 in., the oven features a uniformity of ±15°F between 200°F and 1200°F. Constructed with ceramic fiber insulation for energy savings and faster heating and cooling cycles, the oven includes a stainless steel roller hearth for ease of loading/unloading.

Heating elements located on the side walls are designed from heavy-gauge resistive element wire mounted over ceramic tubes for full radiation from the coils for rapid heat. Each element is mounted individually, reportedly allowing for easy and low-cost replacement. A high-volume stainless steel fan assembly with heat slinger circulates air around the alloy liner, past the heating elements, and through the chamber to provide uniform heat to the workload.

The oven includes a Honeywell over-temperature controller and chart recorder. A safety micro-switch automatically shuts off power to the fan and heating elements when the door is opened.

For more information, visit www.luciferfurnaces.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!