Harper Receives Contract for Pilot-Scale Carbon Fiber Line

Harper International recently announced it has booked a contract for a fully integrated pilot scale carbon fiber conversion line. The line will be installed in Europe to produce carbon fiber for use in advanced communication technology.

The fully integrated line incorporates several progressive design features for the production of carbon fiber from 6K PAN precursor and is engineered for higher than traditional processing speeds. Harper will supply its advanced oxidation oven technology; LT and HT slot furnaces rated for 1000°C and 1600°C, respectively; fiber surface treatment and size application conditioning; waste gas abatement; and material transport systems.

“We are pleased to add this project to our list of Harper-designed, technically advanced complete carbon fiber lines,” said Charles Miller, Jr., president. “Our ongoing string of wins demonstrates the superiority of our technology offering and proven track record, and further reinforces our position as the premiere partner to the industry.”

For more information, visit www.harperintl.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!