Medical Ceramics Market to Reach $13 Billion by 2017

July 7, 2011
/ Print / Reprints /
ShareMore
/ Text Size+

The 2011 global medical ceramics market is estimated at $10.4 billion; the market is projected to increase at a compound annual growth rate (CAGR) of 3.5% (2007-2017) to reach $13.1 billion by 2017. Ceramic technology developments have contributed heavily to the development of implantable electronic devices. According to “Medical Ceramics - A Global Market Overview,” a new report from MarketResearch.com, biocompatibility and resistance to wear have made ceramic materials ideal for a range of medical implant applications, from artificial joints to implantable electronic sensors, stimulators and drug delivery devices.

Alumina and zirconia, among other ceramics, have been successful in holding up to the harsh environment of the human body. The report examines the market for aluminum oxide, zirconia, zirconia alumina and others. In addition, the report includes the market analysis for end-use application areas such as dental, orthopedic, implantable electronic devices, surgical and diagnostic instruments, and others.

For more information, visit www.marketresearch.com/product/display.asp?ProductID=6424613.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

September 2014 Issue Highlights

Our September 2014 issue is now available!

Posted: December 15, 2014

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI December 2014 cover

2014 December

Be sure to check out our annual Services Directory and Business Guide, with additional articles on advanced glass components, ceramic grinding media, and more!

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!