Ceramic Industry News

TA Instruments Acquires Anter Corp. and Anter Laboratories

TA Instruments recently announced it has acquired Anter Corp. and Anter Laboratories, a privately held manufacturer of high-performance systems that measure thermal expansion, thermal conductivity, thermal diffusivity, and heat capacity of a range of materials.

“This acquisition adds powerful technologies that complement TA Instruments’ market-leading thermal analysis product line,” said Terry Kelly, president of TA Instruments. “The combination of TA and Anter technologies and the integration into TA’s worldwide sales and technical support organizations will greatly benefit scientists who need to characterize the thermophysical properties of high-temperature materials.”

Key products developed by Anter include laser and xenon flash systems designed to measure thermal diffusivity and heat capacity of materials up to 2800°C, dilatometer systems to measure thermal expansion, and guarded heat flow meters that measure thermal conductivity of materials in accordance with ASTM standards. Anter systems are used by scientists that develop and characterize ceramics, metals, and glasses for use in a range of industries, including electronics, energy, and aerospace.

For more information, visit www.anter.com or www.tainstruments.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!