Researchers are using a new technology to find out more about 12th century Scottish pottery.

New identification techniques have recently helped researchers find out more about 12th century Scottish pottery. A study funded by Historic Scotland allowed researchers to use inductively coupled plasma mass spectroscopy (ICP-MS) to investigate and define a number of clay sources across Scotland. After examining ceramic fragments from several major abbeys and kiln sites, the research team was able to isolate the distinct sources of production--even those that are just half a mile apart. The information gathered during the study will aid ceramic researchers and Scottish historians in their understanding of ancient pottery.

Historic Scotland is an executive government agency that aims to preserve Scotland's rich historic past and encourage others to understand and enjoy the country's history. For more information, visit www.historic-scotland.gov.uk/index.html.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!