UNION PROCESS: Phosphate Precursor Process

This Akron-based equipment maker has developed a two-phase process for grinding and dispersing the phosphate precursor required for lithium-ion batteries. The first phase uses the company’s S-series attritors to grind and disperse the coarse precursor powder to a 1-3 µm particle size range. The second phase runs through the company’s DMQ series horizontal media mills, dispersing the finished material to a primary particle size range of 200-300 nm.

“Thorough testing of this two-phase method of processing lithium-ion phosphate precursor has shown a high level of repeatability,” said Arno Szegvari, CEO. “As transportation choices become more eco-friendly, we are pleased that we can contribute to the continuing expansion of green technology.”

For more information, visit www.unionprocess.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 February

You won't want to miss this issue, which includes our annual R&D Lab Equipment and Instrumentation Directory!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!