FERRO ELECTRONIC MATERIALS: Silver Conductor Pastes

Two new rear silver conductor pastes are now available. The new products reportedly reduce cost per watt while maintaining the same adhesion, solderability, and field reliability as current commercial products, enabling solar energy to become a more cost-competitive energy generation alternative.

The new pastes have pure silver metallurgy and can enable fast printing at speeds of more than 200 mm per second. They are compatible with the company’s back surface aluminum pastes and can be co-fired in a wide processing window. Both provide robust soldering behavior with excellent adhesion to silicon wafers and have demonstrated field-proven module performance. PS 2130 and PS 2131 silver pastes are RoHS- and REACH-compliant and are free of lead, cadmium, and phthalates.

For more information, visit www.ferro.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!