Zircotec Develops Diesel Engine Barrier Coating

Zircotec recently announced it has developed a new fit-and-forget ceramic coating offering surface temperature reductions of 125°C for diesel engine applications. The new ceramic formulation offers an option for truck and bus manufacturers challenged by the higher temperatures experienced with new Euro VI emissions regulations and testing methods set to be introduced in late 2013.

“Euro VI will require manufacturers to further reduce NOx and particulate matter,” said Peter Whyman, sales director. “There are also changes to the test cycle, including cold start and soak test. During running, engines are running hotter and in these conditions, improved thermal management is likely to help the manufacturers improve performance and overall engine reliability. This is particularly relevant for some after-treatment systems.”

The coating can be applied to exhausts and turbochargers, as well as plastic heatshields, to manage heat, protect other components, and help emissions controls systems work at their optimum.

“From our discussions with engine manufacturers and OEMs, heat management is more crucial with Euro VI,” Whyman said. “Whether this is for SCR engines where getting the catalyst warm is key, or in general terms, the engines are running hotter with heat soak to other components under the engine bay risking poor reliability. We now have a durable, yet cost effective solution and, unlike some lagging products that require reapplication, we can offer reliability throughout the vehicle’s life.”

The coating is applied using plasma spraying, in effect welding the coating to the substrate. It can be applied to most metals, as well as many plastics and composites.

For additional details, visit www.zircotec.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!