QUANTACHROME: Super Carbon

June 16, 2011
/ Print / Reprints /
ShareMore
/ Text Size+

This company’s director of Applied Science, Matthias Thommes, Ph.D., and staff scientist, Katie Cychosz, Ph.D., have collaborated with the University of Texas and Brookhaven National Laboratory to develop a novel micro-mesoporous carbon material, described as exfoliated graphene oxide.

The porous, three-dimensional carbon can reportedly be used as an enhanced supercapacitor, and thus shows promise for many energy storage uses. The new material can be described as an “electrical charge storage sponge” based on its continuous 3-D network of pores with walls just one atom thick. The material’s BET surface area was reported as up to 3100 m2, and it has pores primarily 0.6- 5 nm wide.

For additional details, visit www.quantachrome.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI January 2015 cover

2015 January

It's our annual Materials Handbook issue, with the ever-popular "Raw & Manufactured Materials Overview" article! Check it out today.

Table Of Contents Subscribe

Personal Smartphones

Do you use your personal smartphone or other device to complete tasks for your job?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!