Toshiba America Electronic Components Inc. (TAEC) recently announced it will sell and support the silicon nitride bearing ball blanks and engine components manufactured by Toshiba Materials Co. Ltd. These products, formerly represented by Enceratec, a joint venture of Cummins Inc. and Toshiba Materials Co. Ltd., will now be available direct from TAEC to customers in Europe and North America.

“The addition of Toshiba Material’s silicon nitride bearing blanks product line will complement the diverse collection of other advanced material-based products currently available from TAEC,” said Jim Walker, director of business development with the Advanced Materials Division of TAEC. “Hybrid ball bearings are now being used in a growing number of applications ranging from machine tool spindles and windmills to the main engine turbo pumps on the space shuttle. Hybrid bearings enable rotating machine systems to attain significantly higher speeds and improved reliability, even in lubrication-starved environments.”

For more information, visit www.toshiba.co.jp/index.htm.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!