PPG Industries recently announced it has activated a new 4800-watt solar system at the PPG Glass Business and Discovery Center in Harmar, Pa., near the company’s Pittsburgh headquarters. The system reportedly enables PPG to demonstrate for customers the value of its prototype and existing solar glass products, such as the SOLARPHIRE(R) glass product line, and to help researchers and product developers gather real-world data on the performance of these products.

The center is currently equipped with two 10-module arrays: one using Solarphire PV photovoltaic glass, and one using Solarphire AR anti-reflective glass. Online monitoring software measures the real-time power output of each array, and solar power generated by the system is tied back into building operations.

The site also is available for use by PPG customers to test and demonstrate their products in one-month intervals. Customers with products installed on the array can access performance data via email or the Internet.

For more information, call (412) 820-8500 or visit www.ppg.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

2015 Ceramics Expo

Snapshots from the 2015 Ceramics Expo, April 28-30, Cleveland, Ohio. Posted: May 14, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI May 2015 cover

2015 May

Our May issue covers bulk batching, pneumatic conveyors, high-temperature furnaces and more! Be sure to check it out today.

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!