UNION PROCESS: Metal-Free Attritor

This company recently announced it has built a large SD-250 for an application in the lithium battery industry. The dry grinding SD-250 attritor features a 400 HP TEFC inverter duty motor with a heavy-duty variable-frequency drive controller.

“This is one of the largest and most powerful metal-free attritors we have ever built,” said Emery Li, sales manager. “A steel frame riser was also provided to support and elevate the attritor so that the multiple bottom product discharge valves will be easily accessible for material handling purposes. Noise insulation for the grinding tank was also provided to reduce the dB levels during processing. The high-tech needs of the lithium battery industry require highly engineered equipment. As such, we are proud that Union Process attritors are playing a vital role in the burgeoning green technology market.”

The SD-250 has a gross tank volume of approximately 288 gal, a material capacity of ~125 gal and a media volume of 187 gal. Batch attritors are designed to allow material to be charged into the mill at the top, ground for a predetermined time, then discharged through the bottom.

For more information, visit www.unionprocess.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

October 2014 Issue Highlights

Our October 2014 issue is now available!

Posted: January 29, 2015

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI March 2015 cover

2015 March

We're focusing on thermal processes and decorating in this issue. Check it out!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!