Ceralink Inc. recently announced the opening of a new Materials Testing facility located in St. Clairsville, Ohio. Ceralink Materials Testing (Ceralink MT) will specialize in advanced materials testing services for ceramic matrix composites (CMCs).    

Ceralink MT offers high cycle fatigue testing of CMCs at temperatures up to 2500°F. The new 6,400-sq-ft testing facility houses multiple servo-hydraulic fatigue testing frames and various thermophysical analysis instrumentation. Creep rupture and environmental exposure capabilities will be added as well.

“The addition of Ceralink’s Materials Testing facility allows us to expand our capabilities and respond to customer needs for precision, rapid turnaround CMC testing critical to their development programs,” said Drew Spradling, CTO. “As a company founded and operated by ceramic engineers, we feel we can offer a unique perspective in the testing and evaluation of a wide range of CMC properties.”

For more information, visit www.ceralink.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40