Ceralink Opens Materials Testing Facility

Ceralink Inc. recently announced the opening of a new Materials Testing facility located in St. Clairsville, Ohio. Ceralink Materials Testing (Ceralink MT) will specialize in advanced materials testing services for ceramic matrix composites (CMCs).    

Ceralink MT offers high cycle fatigue testing of CMCs at temperatures up to 2500°F. The new 6,400-sq-ft testing facility houses multiple servo-hydraulic fatigue testing frames and various thermophysical analysis instrumentation. Creep rupture and environmental exposure capabilities will be added as well.

“The addition of Ceralink’s Materials Testing facility allows us to expand our capabilities and respond to customer needs for precision, rapid turnaround CMC testing critical to their development programs,” said Drew Spradling, CTO. “As a company founded and operated by ceramic engineers, we feel we can offer a unique perspective in the testing and evaluation of a wide range of CMC properties.”

For more information, visit www.ceralink.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

November 2014 Issue Highlights

Our November 2014 issue is now available! Posted: March 31, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!