MORGAN THERMAL CERAMICS: Superwool

Superwool® HT™ Felt and Superwool HT™ Millboard are reportedly ideal for fabricating gaskets and heat shields for industrial appliances, including ovens, fryers, and cooking equipment. The lightweight, multi-purpose products are available in a range of sizes, thicknesses and densities, and can offer equivalent performance to traditional refractory ceramic fiber (RCF) insulation in many applications.

As global regulatory restrictions on RCF are being tightened, many manufacturers of industrial appliances around the world are seeking to move toward insulation alternatives. Superwool fiber has been developed to provide the improved high-temperature characteristics required to act as an alternative to RCF. Rigorous testing has established that Superwool fiber products feature low bio-persistence, and felt and millboard made from Superwool fiber are fully exonerated from any carcinogenic classification under nota Q of directive 97/69 EC issued by the European Union. They are not restricted by European REACH (Registration, Evaluation, Authorization and Restriction of Chemical substances) regulations.

For more information, visit www.morgancrucible.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Improving HTCCs and LTCCs
Jim Ellis of Credence Engineering discusses the optimization of ceramic substrates for microelectronics applications.
More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI June 2013 cover

2013 June

The 2013 June Ceramic Industry includes articles on flat boron, decorative tile, patents, OLED lighting, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40