Ceramic Industry News / Advanced Ceramics

Graphene Market to Reach $100 Million by 2018

The market for graphene is expected to reach $100 million by 2018, according to “Graphene: Analysis of Technology, Markets and Players 2013-2018,” a new report from IDTechEx. There are many different types of graphene, each offering a different set of properties. The differentiating parameters include the number of layers, purity, oxygen content, crystallinity and form (powder or sheet). Depending on the specifics of these parameters, the quality of the so-called graphene can vary, from that of the ideal material toward that of graphite oxide.

Each graphene type is manufactured using a different technique; all techniques differ in terms of their cost structure, volume production capability and, ultimately, potential target markets. The manufacturing techniques include micro-cleavage, chemical vapor deposition, liquid-phase exfoliation, oxidization-reduction and plasma.

The main market driver thus far has been the R&D sector. The industry is now gearing up to move beyond research activities and a diverse range of other applications are actively being developed, according to the report. These include RFID, smart packaging, supercapacitors, composites, ITO replacement, sensors, logic and memory.

The strength of graphene’s value proposition is different for each target market. In many cases, graphene enables performance premiums, giving space for premium pricing. Cost will remain critical, however, as graphene’s ultimate value proposition can often only be defined against the incumbent material option.

Composites and energy storage applications are expected to be the largest near-term market opportunity for graphene beyond R&D. Graphene will first penetrate markets that have low cost sensitivity but demand high performance. In the energy storage space, graphene will first be used in supercapacitor devices, mainly due to its high surface-to-volume ratio.

Graphene is forecast to have limited success in the transparent conductor market, because it falls short both on cost and performance compared to incumbent and alternative options. Market success will be limited in the transistor area, both in analogue and digital applications. This is partly due to a lack of bandgap and the high level of standards set by incumbent solutions.

For additional information, visit www.IDTechEx.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

December 2014 Issue Highlights

Our December 2014 issue is now available! Posted: April 27, 2015.

Podcasts

Ceramics Expo podcast
Editor Susan Sutton discusses the upcoming Ceramics Expo with event director Adam Moore.
More Podcasts

Ceramic Industry Magazine

CI April 2015 edition

2015 April

You'll want to check out our continuing coverage of the inaugural Ceramics Expo event, plus articles on dental ceramics, glass coatings, refractories, and more!

Table Of Contents Subscribe

Daily News

We know where you find the latest ceramic industry news (ahem), but where do you catch up on the rest of your daily news?
View Results Poll Archive

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!