Here Comes the Sun

New solar cells could increase the maximum efficiency of solar panels by over 25%, according to researchers from the University of Cambridge. Scientists from theCambridge Cavendish Laboratory in the university’s Department of Physics, have developed a novel type of solar cell that could harvest energy from the sun much more efficiently than traditional designs. The research, published in the journal NanoLetters, could dramatically improve the amount of useful energy created by solar panels.

Solar panels work by absorbing energy from particles of light, called photons, which then generate electrons to create electricity. Traditional solar cells are only capable of capturing part of the light from the sun; much of the energy of the absorbed light, particularly of the blue photons, is lost as heat. This inability to extract the full energy of all of the different colors of light at once means that traditional solar cells are incapable of converting more than 34% of the available sunlight into electrical power.

The Cambridge team, led by professors Neil Greenham and Sir Richard Friend, has developed a hybrid cell that absorbs red light and harnesses the extra energy of blue light to boost the electrical current. Typically, a solar cell generates a single electron for each photon captured. However, by adding pentacene, an organic semiconductor, the solar cells can generate two electrons for every photon from the blue light spectrum. This could enable the cells to capture 44% of the incoming solar energy.
 

“Organic and hybrid solar cells have an advantage over current silicon-based technology because they can be produced in large quantities at low cost by roll-to-roll printing."

Bruno Ehrler, the lead author of the paper, said, “Organic and hybrid solar cells have an advantage over current silicon-based technology because they can be produced in large quantities at low cost by roll-to-roll printing. However, much of the cost of a solar power plant is in the land, labor and installation hardware. As a result, even if organic solar panels are less expensive, we need to improve their efficiency to make them competitive. Otherwise, it’d be like buying a cheap painting, only to find out you need an expensive frame.”

Mark Wilson, another author of the paper, said, “I think it’s very important that we move toward sustainable sources of energy, and it’s exciting to help explore possible solutions.”

“This is just the first step toward a new generation of solar cells, and we are very excited to be a part of this effort,” said Akshay Rao, Ph.D., co-author of the paper.

The research was funded by the Engineering and Physical Sciences Research Council (EPSRC).

For more information, visit www.phy.cam.ac.uk

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Rudy Djaja
October 6, 2012
Looking forward the further possibility to be used in the industry scale.

Multimedia

Videos

Podcasts

Improving HTCCs and LTCCs
Jim Ellis of Credence Engineering discusses the optimization of ceramic substrates for microelectronics applications.
More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI June 2013 cover

2013 June

The 2013 June Ceramic Industry includes articles on flat boron, decorative tile, patents, OLED lighting, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40